Polyester fiber excellent in workability and process for producing same
AssigneeAsahi Kasei Kabushiki Kaisha
InventorsKatsuhiro Fujimoto, Jinichiro Kato
Life of this patent
Estimating the term…
Loading patent…
AssigneeAsahi Kasei Kabushiki Kaisha
InventorsKatsuhiro Fujimoto, Jinichiro Kato
Estimating the term…
A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.: 0.18≦Q/R≦0.45 (1) The polyester fiber of the present invention is a poly(trimethylene terephthalate) fiber which has an elongation, a thermal stress and a boil-off shrinkage in appropriate ranges, and the woven or knitted fabric prepared therefrom shows inhibition of an excessive thermal shrinkage during processing and manifests a low elastic modulus and a soft hand touch. Accordingly, the polyester fiber of the present invention is suitable for use in innerwear, outerwear, sportswear, legwear, lining cloths, swimwear and the like. In addition, the polyester fiber can be stably manufactured in high productivity by a process in which spinning and drawing are consecutively conducted to prevent the undrawn yarn from aging.
A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C., and being wound into a cheese-like package:
A cheese-like package which is formed by winding a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of a thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):
A polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of the thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):
A cheese-like package which is formed by winding a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of the thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2), and which shows a bulging rate of 10% or less:
A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solid filaments, winding the solidified filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.
A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising passing molten filaments extruded from a spinning nozzle through a retarded cooling zone 2 to 80 cm long provided directly below the spinning nozzle and held at atmospheric temperatures of 30 to 200° C., whereby rapid cooling of the filaments is suppressed, rapidly cooling the molten filaments to be changed into solidified filaments, winding the solidified filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.
A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solidified filaments, winding the solid filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, cooling the fiber with a third roll, and winding the fiber on a winder having a peripheral speed lower than that of the second roll.
A process for producing a polyester fiber, wherein a polyester comprising 90% or more by weight of a poly(trimethylene terephthalate) is melt spun, the process comprising rapidly cooling molten filaments extruded from a spinning nozzle to be changed into solidified filaments, imparting a finishing agent to the fiber, whereby the lubricant amount becomes from 0.2 to 3% by weight, winding the solid filaments round a first roll heated at 30 to 80° C. and having a peripheral speed of 300 to 3,500 m/min without winding thereon, winding the filaments round a second roll heated at 100 to 160° C., whereby the filaments are drawn at a draw ratio of 1.3 to 4 between the first and the second roll having a peripheral speed higher than that of the first one, and winding the filaments on a winder having a peripheral speed lower than that of the second roll.
A fabric partly or entirely formed with a polyester fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), and showing a peak value of a thermal stress of 0.1 to 0.35 g/d, a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), and a peak temperature of a loss tangent of 90 to 120° C.:
A fabric partly or entirely formed with a fiber comprising 90% or more by weight of a poly(trimethylene terephthalate), showing a boil-off shrinkage of 5 to 16%, a tenacity of 3 g/d or more, an elongation of 20 to 60%, a relationship between an elastic modulus Q (g/d) and an elastic recovery R (%) satisfying the formula (1), a peak temperature of a loss tangent of 90 to 120° C., a peak temperature of a thermal stress of 100 to 200° C., a peak value of a thermal stress of 0.1 to 0.35 g/d, and a relationship between the peak value of a thermal stress and a thermal stress at 100° C. satisfying the formula (2):