Fire door core
AssigneeGeorgia-Pacific Corporation
InventorDonald F. Klus
Life of this patent
Estimating the term…
Abstract
The present invention describes an improved building material composition, useful for example as a fire door core and to improved methods of making this composition. The building material of the present invention consists essentially of expanded perlite, a fireproof binder, clay or vermiculite, and optionally diatomaceous earth, one or more viscosity-enhancing components, reinforcement fibers, and a plasticizer or mixtures thereof. The method of making this improved composition is a semi-continuous batch press method wherein at least the expanded perlite, fireproof binder, and clay or vermiculite are mixed; the mixture compressed in a mold, and the compressed mixture dried.
Claims37
A building material composition consisting essentially of:
- (a) expanded perlite,
- (b) a fireproof binder,
- (c) clay or vermiculite.
A building material composition consisting essentially of:
- (a) expanded perlite,
- (b) a fireproof binder,
- (c) clay or vermiculite,
- (d) reinforcement fibers, said reinforcement fibers present in an amount of about 0.1 to about 2.0 weight percent of the building material composition.
A building material composition consisting essentially of:
- (a) expanded perlite,
- (b) a fireproof binder,
- (c) clay or vermiculite and
- (d) diatomaceous earth.
A building material composition consisting essentially of:
- (a) expanded perlite,
- (b) a fireproof binder,
- (c) clay or vermiculite
- (d) diatomaceous earth and
- (e) reinforcement fibers.
A fire door core consisting essentially of:
- (a) expanded perlite in an amount from about 50 to about 80 weight percent of said fire door core;
- (b) a fireproof binder in an amount from about 4 to about 19 weight percent of said fire door core;
- (c) clay or vermiculite in an amount from about 2 to about 18 weight percent of said fire door core and
- (d) diatomaceous earth in an amount from about 1 to 10 weight percent of said fire door core.
A fire door core consisting essentially of:
- (a) expanded perlite in an amount from about 50 to about 80 weight percent of said fire door core;
- (b) a fireproof binder in an amount from about 4 to about 19 weight percent of said fire door core;
- (c) clay or vermiculite in an amount from about 2 to about 18 weight percent of said fire door core and
- (d) diatomaceous earth in an amount from about 1 to 10 weight percent of said fire door core and
- (e) reinforcement fibers present in an amount of about 0.1 to about 2.0 weight percent of the composition.
A method of making a building material composition comprising:
- (a) combining expanded perlite, a fireproof binder, diatomaceous earth and clay or vermiculite to form a wet mixture;
- (b) press molding the wet mixture formed in step (a) in a press mold for a time and at a pressure sufficient to bind the mixture together into a wet composite;
- and
- (c) curing the wet composite of step (b) for a time and temperature sufficient to remove substantially all the water from the composite and to form the building material composition.
A method of making a building material composition comprising:
- (a) combining expanded perlite, a fireproof binder, diatomaceous earth, a plasticizer, reinforcement fibers and clay or vermiculite to form an aqueous wet mixture;
- (b) press molding the aqueous wet mixture formed in step (a) in a press mold for a time and at a pressure sufficient to bind the mixture together into a wet composite;
- and
- (c) curing the wet composite of step (b) for a time and temperature sufficient to remove substantially all the water from the composite and to form the building material composition.
Dependencies are inferred from the claim text.