Rare earth magnet and method for manufacturing the same
OwnerFutoshi Kuniyoshi, Hitoshi Morimotoinventors
Life of this patent
Estimating the term…
Abstract
Rare earth alloy powder having an oxygen content of 50 to 4000 wt. ppm and a nitrogen content of 150 to 1500 wt. ppm is compacted by dry pressing to produce a compact. The compact is impregnated with an oil agent and then sintered. The sintering process includes a first step of retaining the compact at a temperature of 700° C. to less than 1000° C. for a period of time of 10 to 420 minutes and a second step of permitting proceeding of sintering at a temperature of 1000° C. to 1200° C. The average crystal grain size of the rare earth magnet after the sintering is controlled to be 3 μm to 9 μm.
Claims15
A method for manufacturing an R—Fe—B rare earth magnet, comprising the steps of:
- a. preparing rare earth alloy powder having an oxygen content in a range of 50 wt. ppm to 4000 wt. ppm and a nitrogen content in a range of 150 wt. ppm to 1500 wt. ppm;
- b. compacting the rare earth alloy powder by dry pressing to produce a compact;
- c. impregnating the compact with an oil agent from the surface of the compact;
- and,
- d. sintering the compact,
- wherein the step of sintering the compact includes:
- a first step of retaining the compact at a temperature in a range of 700° C. to less than 1000° C. for a period of time in a range of 10 minutes to 420 minutes;
- and
- a second step of permitting proceeding of sintering at a temperature in a range of 1000° C. to 1200° C., and the average crystal grain size of the rare earth magnet after the sintering is in a range of 3 μm to 9 μm.
An R—Fe—B rare earth magnet, having an average crystal grain size in a range of 3 μm to 9 μm, an oxygen concentration in a range of 50 wt. ppm to 4000 wt. ppm, and a nitrogen concentration in a range of 150 wt. ppm to 1500 wt ppm.
A method for manufacturing an R—Fe—B rare earth magnet, comprising the steps of:
- a. preparing rare earth alloy powder having an oxygen content in a range of 50 wt. ppm to 4000 wt. ppm and a nitrogen content in a range of 150 wt. ppm to 1500 wt. ppm by embrittling an R—Fe—B rare earth alloy by hydrogen occlusion and milling the embrittled alloy;
- b. compacting the rare earth alloy powder to produce a compact;
- c. retaining the compact at a temperature in a range of 700° C. to less than 1000° C. for a period of time in a range of 10 minutes to 420 minutes and releasing hydrogen outside the compact so that the amount of hydrogen contained in sintered magnet is in a range of 10 wt. ppm to 100 wt. ppm;
- and
- d. sintering the compact at a temperature in a range of 1000° C. to 1200° C., wherein the rare earth magnet after the sintering the rare earth magnet has an average crystal grain size in a range of 3 μm to 13 μm and a hydrogen content in a range of 10 wt. ppm to 100 wt. ppm.
An R—Fe—B rare earth magnet, having an oxygen concentration in a range of 50 wt. ppm to 4000 wt. ppm, a nitrogen concentration in a range of 150 wt. ppm to 1500 wt. ppm, and a hydrogen content in a range of 10 wt. ppm to 100 wt.
An R—Fe—B rare earth magnet, having an oxygen concentration in a range of 50 wt. ppm to 4000 wt. ppm, and a hydrogen content in a range of 10 wt. ppm to 100 wt. ppm, wherein a rare earth element concentration is 32 wt. % or less of the magnet.
Dependencies are inferred from the claim text.