Abstract
The present invention provides a method of steam reforming a hydrocarbon over a spinel-containing catalyst at short residence times or short contact times. The present invention also provides spinel-containing catalysts. Surprisingly superior results and properties obtained in methods and catalysts of the present invention are also described.
Claims18
A method of steam reforming, comprising:
- passing steam and hydrocarbon through a reaction chamber;
- wherein the reaction chamber comprises a spinel-containing catalyst that has surface active sites comprising a material selected from the group consisting of rhodium, iridium, nickel, palladium, platinum, ruthenium, carbide of group IVb and combinations thereof;
- wherein the rate of said passing steam and hydrocarbon is controlled such that residence time in the reaction chamber is less than 0.1 seconds;
- wherein the temperature in the reaction chamber is in the range of 500° C. to 1000° C.;
- wherein, after passing through the reaction chamber, at least 60% of said hydrocarbon has been converted has been converted to products after passing through the reaction chamber.
2 more elements
A catalyst, comprising:
- (a) a first porous structure with a first pore surface area and a first pore size of at least about 0.1 μm;
- (b) a porous interfacial layer that comprises a spinel with a second pore surface area and a second pore size less than said first pore size, said porous interfacial layer having a thickness less than 4 mm disposed upon said porous structure;
- (c) a steam reforming catalyst selected from the group consisting of rhodium, iridium, nickel, palladium, platinum, ruthenium, carbide of group IVb and combinations thereof disposed upon the second pore surface area.
A catalyst comprising:
- an alumina layer;
- a metal exposed on the surface of the catalyst;
- a spinel layer disposed between the alumina layer and the metal;
- wherein the spinel layer is in direct contact with the alumina layer;
- and
- wherein the metal comprises a metal selected from the group consisting of:
- rhodium, iridium, nickel, platinum, palladium, and ruthenium.