Member made of carbon having layer for protective layer formation and method for producing the same
AssigneeNGK Insulators, Ltd.
InventorsShigeru Hanzawa, Kenji Nakano
Life of this patent
Estimating the term…
Loading patent…
AssigneeNGK Insulators, Ltd.
InventorsShigeru Hanzawa, Kenji Nakano
Estimating the term…
To provide a member made of carbon having a layer for forming a protective layer as an oxidation resistant protective layer and characterized in that a protective layer with a prescribed thickness and high wear resistance and practically resistant against oxidation even at 700° C., preferably 1000° C. or higher, in an atmosphere with a dew point as high as 30 to 70° C. or in the atmospheric air can be formed only in the surface layer part and to provide a method for producing the same member made of carbon. A member made of carbon having a layer for forming a protective layer as an oxidation resistant protective layer is made available by a method wherein carbon paper impregnated with a phenol resin is rolled on the surface of a member made of carbon and after curing the phenol resin or without curing the phenol resin, the resultant member is preferred at 500 to 600° C. in an inert atmosphere to carbonize the phenol resin and to form the layer for the forming a protective layer as the oxidation resistant protective layer of silicon carbide and a method for producing such a member comprises steps of the foregoing steps.
A member made of carbon having a layer for forming a protective layer as an oxidation resistant protective layer.
A method for producing a member made of carbon having a layer for forming a protective layer as an oxidation resistant protective layer of silicon carbide, which comprises steps of forming the layer for forming a protective layer as the oxidation resistant protective layer made of silicon carbide by rolling carbon paper impregnated with a phenol resin on the surface of a member made of carbon, either curing the phenol resin or without curing it, prefiring the phenol resin at 500 to 600° C. in an inert atmosphere, and carbonizing the phenol resin.
Dependencies are inferred from the claim text.