Back to results
US 2001/0025077 A1Published application
Method of producing aqueous dispersions as a base for hot sealing adhesives
AssigneeRoehm GmbH Chemische Fabrik
InventorsHubert Scheuermann, Dieter Tessmer, Karl Foelsch, Wilhelm Elser, Michael Wicke
Life of this patent
Estimating the term…
Abstract
Poly(meth)acrylate dispersions, comprised of: (A) 50-90 wt. % methacrylic acid esters; (B) 5-30 wt. % acrylic acid alkyl esters [lit., “acrylic acid acrylic esters”]; (C) 2-10 wt. % of another functionalized monomer; (D) 2-10 wt. % of a radically polymerizable carboxylic acid or a polycarboxylic acid or a partially esterified polycarboxylic acid; and (E) 0-40 wt. % of a monomer which is copolymerizable with components (A) to (D).
Claims18
Aqueous poly(meth)acrylate dispersions, comprising:
- a particulate poly(meth)acrylate comprising the following components:
- (A) 50-90 wt. % of methacrylic acid alkyl esters;
- (B) 5-30 wt. % of an acrylic acid alkyl ester having a glass transition temperature Tg in the range c. −20 to 50° C. and having formula I:
- 4
- wherein R1 represents an alkyl, aryl, or alkaryl group having 2-10 C atoms;
- (C) 2-10 wt. % of a functionalized monomer of formula II:
- 5
- wherein R2 represents hydrogen or methyl;
- and R3 represents a glycidyl group 6
- or an alkyl group which has 2-6 C atoms and is substituted with at least one hydroxyl group;
- (D) 2-10 wt. % of at least one radically polymerizable carboxylic acid or a polycarboxylic acid or a partially esterified polycarboxylic acid;
- and
- (E) 0-40 wt. % of other monomers which are copolymerizable with (A) to (D);
- wherewith, in the process of preparation, a first polymerization stage (Process Step 1) is conducted with monomers of groups (A) to (C) and optionally (E), and in a second polymerization stage (Process Step 2), monomers of groups (A), (B), (D), and optionally (E) are copolymerized;
- and wherewith the sum of the amounts of monomers (A) to (E) is 100 wt. %.
12 more elements
Aqueous poly(meth)acrylate dispersions, comprising:
- a particulate poly(meth)acrylate comprising the following components:
- (A) 60-80 wt. % of methacrylic acid alkyl esters;
- and
- (B) 10-20 wt. % of an acrylic acid alkyl ester having a glass transition temperature Tg in the range of about −20 to 50° C., of formula I:
- 7
- where R1 represents an alkyl, aryl, or alkaryl group having 2-10 C atoms;
- and
- (C) 3-10 wt. % of a functionalized monomer of formula II:
- 8
- where R2 represents hydrogen or methyl, and
- R3 represents a glycidyl group 9
- or an alkyl group which has 2-6 C atoms and is substituted with at least one hydroxyl group;
- and
- (D) 3-10 wt. % of at least one radically polymerizable carboxylic acid or a polycarboxylic acid or a partially esterified polycarboxylic acid;
- and
- (E) 0-40 wt. % of other monomers which are copolymerizable with (A) to (D);
- wherewith, in the process of preparation,a first polymerization stage (Process Step 1) is conducted of monomers of groups (A) to (C) and optionally (E), and in the second polymerization stage (Process Step 2), monomers of groups (A), (B), (D), and optionally (E) are copolymerized;
- and wherewith the sum of the amounts of monomers (A) to (E) is 100 wt. %.
15 more elements
Dependencies are inferred from the claim text.