Radiation-curable optical fiber coatings having reduced yellowing and fast cure speed
AssigneeDsm N.V.
InventorsDavid M. Szum, Chander P. Chawla, Timothy E. Bishop
Life of this patent
Estimating the term…
Abstract
Radiation-curable inner and outer primary optical fiber coatings are disclosed having both fast cure speed and reduced rates of yellowing. The compositions comprise particular photoinitiators and UV absorbers which are used in amounts to provide the combination of properties. The UV absorber can have ethylenic unsaturation. Outer primary coatings can be formulated to screen inner primary coatings and have fast cure speed.
Claims20
A radiation-curable composition for an optical fiber coating comprising the combination of pre-mixture ingredients:
- about 5 wt. % to about 95 wt. % of at least one radiation-curable oligomer,
- about 5 wt. % to about 95 wt. % of at least one reactive diluent,
- about 0.1 wt. % to about 20 wt. % of at least one photoinitiator, wherein said photoinitiator is selected to provide a fast cure speed,
- about 0.1 wt. % to about 20 wt. % of at least one UV absorbing compound which does not substantially impair said fast cure speed.
A radiation-curable composition for an optical fiber coating comprising the combination of pre-mixture ingredients:
- about 5 wt. % to about 95 wt. % of at least one radiation-curable urethane acrylate oligomer,
- about 5 wt. % to about 95 wt. % of at least two reactive diluents comprising acrylate functionality,
- about 0.1 wt. % to about 20 wt. % of at least one phosphine oxide photoinitiator,
- about 0.1 wt. % to about 20 wt. % of at least one UV absorbing compound which comprises an acrylate functionality.
A coated optical fiber comprising the combination of:
- an optical fiber,
- a radiation-cured inner primary optical fiber coating, and
- a radiation-cured outer primary optical fiber coating, wherein
- said outer primary optical fiber coating comprises, before radiation-cure, the combination of pre-mixture ingredients:
- about 5 wt. % to about 95 wt. % of at least one radiation-curable oligomer,
- about 5 wt. % to about 95 wt. % of at least one reactive diluent,
- about 0.1 wt. % to about 20 wt. % of at least one photoinitiator, wherein said photoinitiator is selected to provide a fast cure speed,
- about 0.1 wt. % to about 20 wt. % of at least one UV absorbing compound which does not substantially impair the fast cure speed of the inner or outer primary coating.
A method for reducing the rate of color degradation in an inner primary optical fiber coating comprising the combination of steps of:
- coating an optical fiber with a radiation-curable inner primary coating,
- coating said inner primary coating with a radiation-curable outer primary coating which comprises a UV absorber which does not substantially impair the cure speed of the outer primary coating,
- radiation-curing said coatings.
Dependencies are inferred from the claim text.