Systems and methods for on/off leaching of a heap
AssigneeFreeport Minerals Corporation
InventorsCristian Alejandro Caro, Adam John Leonard, Vladimir Antonio Ancasi Huisa
Life of this patent
Estimating the term…
Abstract
Methods for recovering a metal value from a metal-bearing material are provided. The method comprises intermittent application of a heated leaching solution to a plurality of regions of the metal bearing material followed by a period of time where no additional heating leaching solution is applied. This method results in a cyclical heating pattern that improves recovery of the metal value with reduced energy and reagent expenditure.
Claims20
A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
- defining a plurality of regions within the metal-bearing material;
- applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
- wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature above an ambient temperature of the first region of the metal-bearing material,
- wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of the ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
- waiting for a first period of time,
- wherein, during the first period of time at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a first amount of a pregnant leaching solution,
- wherein during the first period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
- wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the first period of time;
- and wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value.
A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
- defining a plurality of regions within the metal-bearing material;
- applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
- wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature above an ambient temperature of the first region of the metal-bearing material,
- wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of the ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
- waiting for a period of time between about 30 and about 60 days,
- wherein, during the period of time at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a first amount of a pregnant leaching solution,
- wherein during the period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
- wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the period of time;
- and
- wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value.
A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
- defining a plurality of regions within the metal-bearing material;
- applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
- wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature between about 40° C. and about 50° C.,
- wherein the first amount of heated leaching solution is applied over a period time of about 30 to about 60 days at a rate of between about 5 liters per hour per square meter and about 10 liters per hour per square meter,
- wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of an ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
- terminating application of the heated leaching solution to the first region of the metal-bearing material;
- waiting for a period of time between about 30 and about 60 days,
- wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the period of time;
- wherein during the period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
- wherein, during the application and waiting periods, at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a pregnant leaching solution,
- optionally repeating the application, termination, and waiting steps a plurality of times;
- and
- collecting the pregnant leaching solution,
- wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value and/or wherein energy and reagent expenditure is less than energy and reagent expenditure realized when heated leaching solution is constantly applied to the metal-bearing material for an equivalent period of time.
Dependencies are inferred from the claim text.