Back to results
US 12,703,898 B2Granted
MCrAlX-alloy, powder, coating for protection against corrosion and oxidation and for bonding ceramic insulating coating and component
AssigneeSiemens Energy Global GmbH & Co. KG
InventorsXin-Hai Li, Snezana Djordjevic
Life of this patent
Estimating the term…
Abstract
A MCrAlX-alloy, powder, coating for protection against corrosion and oxidation and for bonding ceramic insulating coating and component. The nickel-based alloy NiCoCrAlY includes: Cobalt (Co) 24.5%-26.5%; Chrome (Cr) 14.5%-16.5%; Aluminum (Al) 11.6%-12.6%; Yttrium (Y) 0.3%-0.5%; Iron (Fe) 4.0%-5.0%; Tantalum (Ta) 0.6%-0.8%; Molybdenum (Mo) 0.4%-0.6%; Silicon (Si) 0.4%-0.6%.
Claims9
A nickel-based alloy, consisting of (in wt %):
- Cobalt (Co)
- 25.5%
- Chrome (Cr)
- 15.5%
- Aluminum (Al)
- 12.1%
- Iron (Fe)
- 4.5%
- Tantalum (Ta)
- 0.7%,
- Molybdenum (Mo)
- 0.5%
- Silicon (Si)
- 0.5%
- Sulfur (S)
- ≤10 ppm,
- no Rhenium (Re) or Ruthenium (Ru), and a balance of Nickel (Ni).
14 more elements
A nickel-based alloy, consisting of (in wt %):
- Cobalt (Co)
- 24.5%-26.5%
- Chrome (Cr)
- 14.5%-16.5%
- Aluminum (Al)
- 11.6%-12.6%
- Hafnium (Hf)
- 0.3%-0.5%
- Iron (Fe)
- 4.0%-5.0%
- Tantalum (Ta)
- 0.6%-0.8%
- Molybdenum (Mo)
- 0.4%-0.6%
- Silicon (Si)
- 0.4%-0.6%
- Sulfur (S)
- ≤10 ppm,
- no Rhenium (Re) or Ruthenium (Ru), and a balance of Nickel (Ni).
16 more elements
A nickel-based alloy, consisting of (in wt %):
- Cobalt (Co)
- 24.5%-26.5%
- Chrome (Cr)
- 14.5%-16.5%
- Aluminum (Al)
- 11.6%-12.6%
- Iron (Fe)
- 4.0%-5.0%
- Tantalum (Ta)
- 0.6%-0.8%
- Molybdenum (Mo)
- 0.4%-0.6%
- Silicon (Si)
- 0.4%-0.6%
- Sulfur (S)
- ≤10 ppm,
- no Rhenium (Re) or Ruthenium (Ru), and a balance of Nickel (Ni).
14 more elements
Dependencies are inferred from the claim text.