A method of manufacturing steel strip including the steps of: casting molten steel into slabs; reheating the slabs at 1150° C. or more for 1 hour or more; hot rolling the steel into a strip, preferably with an average F1 slab entry temperature above 1000° C.; coiling the hot rolled steel strip; batch annealing the steel strip: at an intercritical temperature (i.e. between Ac1 and Ac3), preferably below 700° C.; in non-oxidising and non-nitrogenated atmosphere; total annealing time at least 5 hours, preferably at least 10 hours to get Mn enrichment in austenite such that Mn content is at least 1.25 times bulk Mn content of the steel and C enrichment such that C content is at least 1.2 times bulk C content of the steel; cooling the steel after batch annealing in air, forced air or water quench.
A method of manufacturing a cold rolled and annealed steel strip, composition of the steel being in wt. %:
Dependencies are inferred from the claim text.