Net for aquaculture
AssigneeAvient Protective Materials B.V.
InventorsHans Schneiders, Bart Tacken
Life of this patent
Estimating the term…
Abstract
Nets, preferably nets for aquaculture are provided, wherein the net comprises cords joined in a net mesh, wherein each cord comprises one or more yarns, the yarns having a tenacity of at least 0.6 N/tex and wherein the net has a mesh size of at least 8 mm, characterized in that the cords further comprise a polymeric resin, wherein the polymeric resin is a homopolymer or copolymer of ethylene and/or propylene, wherein the polymeric resin has a density as measured according to ISO1183 in the range from 860 to 970 kg/m3, a melting temperature in the range from 40 to 140° C. and a heat of fusion of at least 5 J/g. The invention further relates to a fishing net, a fish farming construction comprising said net, a fish farm, and a method for fish farming.
Claims20
A net comprising cords joined in a net mesh, wherein
- the cords in the net mesh are joined by knots such that the net mesh has a mesh size of at least 8 mm as measured from center to center of 2 adjacent knots of the net mesh, and wherein
- each cord comprises one or more yarns, wherein the yarns comprise fibers formed of ultrahigh molecular weight (UHMWPE) fibers, and wherein the yarns have a tenacity of at least 0.6 N/tex as measured according to ASTM D885M, and wherein
- the cords further comprise a polymeric resin which impregnates the one or more yarns throughout a cross-section thereof such that the polymeric resin is present between substantially all of the fibers of the one or more yarns and in contact with at least 70% of surfaces of the fibers of the one or more yarns, and wherein
- the polymeric resin is a homopolymer or copolymer of ethylene and/or propylene, wherein the polymeric resin has a density as measured according to ISO1183-2004 in the range from 860 to 970 kg/m3, a peak melting temperature measured according to ASTM E794-06 in the range from 40 to 140° C. and a heat of fusion of at least 5 J/g measured according to ASTM E793-85 considering the second heating curve at a heating rate of 10 K/min, on a dry sample.