Compositions including a filler, an emissivity agent, a crosslinking facilitator, and a metal silicate binder are disclosed. The compositions can be curable at ambient conditions. Methods of coating overhead conductor and power transmission line accessories with such coating compositions are also disclosed.
Claims18
A method of coating an overhead conductor, comprising:
- providing a coating composition formed from a first part and a second part, wherein the first part comprises a filler, an emissivity agent, and a crosslinking facilitator comprising a latent acid compound, wherein the latent acid compound comprises condensed aluminum phosphate;
- and wherein the second part comprises a metal silicate binder;
- applying the coating composition onto an outer surface of the overhead conductor;
- and
- curing the coating composition at a temperature of from about 15° C. to about 40° C. to form a coated overhead conductor having a cured coating on the outer surface thereof;
- and
- wherein the composition comprises:
- about 35% to about 45%, by dry weight, of the filler;
- about 15% to about 22%, by dry weight, of the emissivity agent;
- about 4% to about 10%, by dry weight, of the crosslinking facilitator;
- and
- about 25% to about 40%, by dry weight, of the metal silicate binder.
9 more elements
A method of coating an overhead conductor, comprising:
- providing a coating composition comprising:
- about 35% to about 45%, by dry weight, of a filler;
- about 15% to about 22%, by dry weight, of an emissivity agent;
- about 4% to about 10%, by dry weight, of a crosslinking facilitator comprising a latent acid compound;
- wherein the latent acid compound comprises condensed aluminum phosphate and
- about 25% to about 40%, by dry weight, of a metal silicate binder;
- wherein the composition comprises the crosslinking facilitator at about 10% to about 30% by weight of the metal silicate binder;
- applying the coating composition onto an outer surface of the overhead conductor;
- and
- curing the coating composition at a temperature of from about 15° C. to about 40° C. to form a coated overhead conductor having a cured coating on the outer surface thereof, wherein curing the coating composition comprises allowing the composition to cure and dry under ambient conditions;
- wherein the coated overhead conductor passes a 1 inch mandrel bend test after immersion in water at 30° C. for 7 days, such that the coating shows no visible cracks when bent on a mandrel having a diameter of 1 inch.
8 more elements