Method of manufacturing merged PiN Schottky (MPS) diode
AssigneeLEAP Semiconductor Corp.
InventorsWei-Fan Chen, Kuo-Chi Tsai
Life of this patent
Estimating the term…
Loading patent…
AssigneeLEAP Semiconductor Corp.
InventorsWei-Fan Chen, Kuo-Chi Tsai
Estimating the term…
A merged PiN Schottky (MPS) diode includes a substrate, a first epitaxial layer of a first conductivity type, doped regions of a second conductivity type, a second epitaxial layer of the first conductivity type, and a Schottky metal layer. The first epitaxial layer is disposed on the first surface of the substrate. The doped regions are disposed in a surface of the first epitaxial layer, wherein the doped regions consist of first portions and second portions, the first portions are electrically floating, and the second portions are electrically connected to a top metal. The second epitaxial layer is disposed on the surface of the first epitaxial layer, wherein trenches are formed in the second epitaxial layer to expose the second portions of the doped regions. The Schottky metal layer is conformally deposited on the second epitaxial layer and the exposed second portions of the doped regions.
A method of manufacturing a merged PiN Schottky (MPS) diode, comprising:
Dependencies are inferred from the claim text.