Glass articles with mixed polymer and metal oxide coatings
AssigneeCorning Incorporated
InventorsDavid Henry, Valerie Claudine Lacarriere
Life of this patent
Estimating the term…
Abstract
According to one or more embodiments, a pharmaceutical package may include a glass container and a coating. The glass container may include a first surface and a second surface opposite the first surface. The first surface may be an outer surface of the glass container. The coating may be positioned over at least a portion of the first surface of the glass container. The coating may include one or more polyimide compositions and one or more metal oxide compositions. The one or more polyimide compositions and the one or more metal oxide compositions may be mixed in the coating.
Claims5
A pharmaceutical package comprising:
- a glass container comprising a first surface and a second surface opposite the first surface, wherein the first surface is an outer surface of the glass container;
- and
- a coating positioned on and in direct contact with at least a portion of the first surface of the glass container, the coating comprising:
- a fluorinated polyimide copolymer formed from a dianhydride monomer component and a diamine monomer component, wherein the dianhydride monomer component is 2,2-bis(3,4-dicarboxyphenyl)hexafluoropropane dianhydride (6FDA), and the diamine monomer component is selected from the group consisting of (i) 1,4-phenylenediamine (mPDA) and 1,3-phenylenediamine (pPDA);
- (ii) 4,4′-oxydianiline (ODA);
- (iii) 4,4′-(2,2,2-trifluoro(1-trifluoromethyl)ethylidene)bisbenzeneamine (4,4′-6F);
- (iv) 3,3′-(2,2,2-trifluoro(1-trifluoromethyl)ethylidene)bisbenzeneamine (3,3′-6F);
- (v) 2,3,5,6-tetramethylphenylene;
- and (vi) 2,2,-bis[4-(4-aminophenoxy)phenyl] hexafluoropropane (4BDAF);
- and
- from 35.8 wt. % to 94.8 wt. % alumina;
- wherein:
- the fluorinated polyimide copolymer and the alumina are mixed in the coating;
- the coating has a thickness of 100 nm or less;
- the combination of the fluorinated polyimide copolymer and alumina comprise at least 99.5 wt. % of the coating;
- the portion of the first surface of the glass container with the coating has a coefficient of friction of less than or equal to about 0.5;
- and
- the portion of the first surface of the glass container with the coating retains the coefficient of friction of less than or equal to about 0.5 following a heat treatment at a temperature of at least about 300° C. for about 30 minutes.
Dependencies are inferred from the claim text.