Back to results
US 11,312,043 B2Granted
Processing additives and uses of same in rotational molding
AssigneeCytec Technology Corp.
InventorsRam Gupta, Sari-Beth Samuels, Thomas Steele, J. Mon Hei Eng
Life of this patent
Estimating the term…
Abstract
The cycle time of polymer compositions subjected to a rotomolding process is improved (i.e., reduced), while the processing window is simultaneously enlarged through the use of a polymer-stabilizing amount of a processing stabilizer system having at least one chroman-based compound according to Formula V:
Claims8
A process for producing a stabilized polymeric hollow article in a rotational molding operation, the process comprising:
- a) filling a mold with a polyolefin and 0.01 to 10% by weight of the total weight of the polyolefin of a stabilizer composition, wherein said stabilizer composition comprises:
- i) vitamin E acetate;
- ii) a phosphite or phosphonite compound;
- and
- iii) at least one basic co-additive selected from calcium stearate, zinc stearate, magnesium behenate, magnesium stearate, sodium ricinoleate, or potassium palmitate;
- b) rotating the mold around at least one axis while heating the mold in an oven for a time interval sufficient to achieve sintering and laydown of the polyolefin, thereby spreading the polyolefin to the walls of the mold;
- c) cooling the heated mold;
- and
- d) opening the mold to remove a resulting product in the form of a stabilized polymeric hollow article;
- wherein the polyolefin comprises linear low density polyethylene (LLDPE), medium density polyethylene (MDPE), high density polyethylene (HDPE), or polypropylene;
- and
- wherein the polyolefin, phosphite or phosphonite compound, and at least one basic co-additive, and amounts of the vitamin E acetate, phosphite or phosphonite compound, and at least one basic co-additive are selected to reach maximum mean failure energy (MFE) of the article at a shorter time interval of the rotational molding operation, to retain a higher MFE of the article over a longer heating time of the rotational molding operation, and to enlarge a processing window of the rotational molding operation to a peak internal air temperature (PIAT) of up to 452° F. with yellowness index of the article remaining substantially unchanged up to a PIAT of 452° F., even in the absence of a sterically hindered amine light stabilizer (HALS).
9 more elements
Dependencies are inferred from the claim text.