Precursor materials for li-ion battery cathode synthesis
AssigneeCAMX Power LLC
InventorsAdrian W. Pullen, Suresh Sriramulu
Life of this patent
Estimating the term…
Loading patent…
AssigneeCAMX Power LLC
InventorsAdrian W. Pullen, Suresh Sriramulu
Estimating the term…
Provided are particles for use as a precursor material for synthesis of Li-ion cathode active material of a lithium-ion cell comprising: a non-lithiated nickel oxide particle of the formula MOx wherein M comprises 80 at % Ni or greater and wherein x is 0.7 to 1.2, M optionally excluding boron in the MOx crystal structure; and a modifier oxide intermixed with, coated on, present within, or combinations thereof the non-lithiated nickel oxide particle, wherein the modifier oxide is associated with the non-lithiated nickel oxide such that a calcination at 500 degrees Celsius for 2 hours results in crystallite growth measured by XRD of 2 nanometers or less. Also provided are processes of forming electrochemically active particles using the precursors nickel oxides.
A particle for use as a precursor material for synthesis of Li-ion cathode active material of a lithium-ion cell comprising:
Dependencies are inferred from the claim text.