A positive electrode material for a nonaqueous electrolyte secondary battery, which comprises a mixture containing a lithium metal composite oxide represented by a general formula LiaNi1-x-y-zCoxMnyMzO2 (wherein, 0.03≤x0.35, 0≤y≤0.35, 0≤z≤0.05, 0.97≤a≤1.30, and M is at least one element selected from V, Fe, Cu, Mg, Mo, Nb, Ti, Zr, W and Al), and an ammonium tungstate powder, wherein
- the positive electrode material is characterized such that when 5 g of the positive electrode material is mixed with 100 ml of pure water, the mixture is stirred for 10 minutes and then left to stand for 30 minutes, and then the pH of a supernatant fluid at 25° C. is measured, the pH ranges from 11.2 to 11.8.