Thermal treatment method for aluminum alloy cast-spun wheel
AssigneeCITIC Dicastal Co., Ltd.
InventorsZuo Xu, Guoyuan Xiong, Honglei Liu, Hongfeng Liu, Rui Wang, Changhai Li
Life of this patent
Estimating the term…
Loading patent…
AssigneeCITIC Dicastal Co., Ltd.
InventorsZuo Xu, Guoyuan Xiong, Honglei Liu, Hongfeng Liu, Rui Wang, Changhai Li
Estimating the term…
A thermal treatment method for an A356 aluminum alloy cast-spun wheel is provided. The thermal treatment method is characterized by including the steps of: 1) heating an aluminum alloy wheel cast-spun piece to 540-550° C.; 2) preserving the heat of the aluminum alloy wheel cast-spun piece for 275-285 minutes at the temperature of 540-550° C.; 3) quenching the aluminum alloy wheel cast-spun piece in water of 70-90° C. for 180 seconds; 4) heating the aluminum alloy wheel cast-spun piece to 150-160° C.; 5) preserving the heat of the aluminum alloy wheel cast-spun piece for 175-185 minutes at 150-160° C.; and 6) cooling the aluminum alloy wheel cast-spun piece in air to room temperature.
A thermal treatment method for an aluminum alloy wheel produced by casting and spinning, comprising the steps of:
Dependencies are inferred from the claim text.