Carbogel anode materials and method for their preperation
AssigneeUniwersytet Jagiellonski
InventorsMonika Bakierska, Marcin Molenda, Agnieszka Chojnacka, Michal Swietoslawski
Life of this patent
Estimating the term…
Abstract
Carbogel anode materials and method for their preparation are disclosed. The described carbogels exhibit, at a temperature of 20° C., an electrical conductance of at least 0.5 S/cm and a reversible electrochemical capacity in relation to lithium of at least 350 mAh/g under a C/2 discharge current, enabling their use for preparation of anode materials, particularly those intended for preparation of lithium-ion cells.
Claims18
A carbogel comprising at least 92% by wt. of carbon and exhibiting, at a temperature of 20° C., an electrical conductance of at least 0.5 S/cm and a reversible electrochemical capacity in relation to lithium of at least 350 mAh/g under a C/2 discharge current;
- wherein the carbogel is prepared by a method comprising the steps of:
- subjecting an aqueous suspension comprising 1-30% by wt. of a first starch composition consisting of rice starch in the amount of 75-99% by wt. and a second starch type in the amount of 1-25% by wt. to polycondensation at a temperature of 50-90° C.;
- carrying out a solvent exchange using an aqueous solutions of an alcohol or a ketone with a concentration increasing from 10% to 99.8% to obtain an organic alcogel, and
- subjecting the obtained organic alcogel to a pyrolysis process at a temperature of 300-2000° C. immediately following the solvent exchange step.
An anode material made from a carbogel for use in a lithium-ion cell, the carbogel comprising:
- at least 92% by wt. of carbon;
- and
- exhibiting, at a temperature of 20° C., an electrical conductance of at least 0.5 S/cm and a reversible electrochemical capacity in relation to lithium of at least 350 mAh/g under a C/2 discharge current;
- and wherein
- the carbogel is prepared by a method comprising the steps of:
- subjecting an aqueous suspension comprising 1-30% by wt. of a first starch composition consisting of rice starch in the amount of 75-99% by wt. and a second starch type in the amount of 1-25% by wt. to polycondensation at a temperature of 50-90° C.;
- carrying out a solvent exchange using an aqueous solutions of an alcohol or a ketone with a concentration increasing from 10% to 99.8% to obtain an organic alcogel, and
- subjecting the obtained organic alcogel to a pyrolysis process at a temperature of 300-2000° C. immediately following the solvent exchange step.
Dependencies are inferred from the claim text.