An abrasive slurry composition for chemical mechanical planarization/polishing (CMP) is provided. The abrasive slurry includes colloidal alumina, a dispersant, and a pH buffer. The colloidal alumina has a particle size of between about 5 nm and about 100 nm. The colloidal alumina may be alpha phase material having a first hardness of about 9 Mohs, or gamma phase material having a second hardness of about 8 Mohs. The abrasive slurry may further include polyacrylic acid (PAA), a down-force enhancer, or a polish-rate inhibitor.
Claims20
A method comprising:
- introducing a slurry to a chemical mechanical polishing pad, the slurry comprising colloidal alumina, wherein the alumina is formed using a sol-gel process, the sol-gel process utilizing β-alanine;
- and
- polishing a semiconductor device layer with the slurry and the chemical mechanical polishing pad.
A method comprising:
- forming colloidal alumina using a sol-gel process, the sol-gel process using AlCl3 and Al(NO3)3 as precursors along with β-alanine, wherein the AlCl3 and Al(NO3)3 are in a ratio of 0.1˜5% and wherein a product is hydrothermally treated at a temperature range of between about 600° C. and about 800° C. for a duration of time between about 1 hour and about 2 hours;
- attaching a semiconductor device wafer to a chemical mechanical planarization (CMP) carrier head;
- introducing a CMP slurry to an exposed surface of the semiconductor device wafer, the CMP slurry comprising the colloidal alumina;
- and
- after introducing the CMP slurry, polishing the exposed surface of the semiconductor device wafer until the semiconductor device wafer has a topological difference spanning a range of about 50 Å.
A method comprising:
- forming a chemical mechanical polishing slurry comprising:
- placing a reactant into a solvent such that the reactant is present between about 0.001%-wt and about 1.5%-wt;
- forming a sol-gel formed colloidal alumina utilizing β-alanine;
- placing the a sol-gel formed colloidal alumina into the solvent, wherein the sol-gel formed colloidal alumina is present between about 0.1%-wt and about 4%-wt;
- and
- placing a dispersant into the solvent such that the dispersant is present between about 0.001%-wt and about 0.1%-wt;
- placing a pH adjustor into the solvent such that the pH adjustor is present between about 0.001%-wt and about 0.1%-wt;
- placing a corrosion inhibitor into the solvent such that the corrosion inhibitor is present between about 0.001%-wt to about 0.1%-wt;
- and
- placing a chelate into the solvent such that the chelate is present between about 0.001%-wt and about 0.01%-wt, wherein the solvent is present between about 95%-wt and about 99%-wt.