High temperature glass melting vessel
AssigneeCorning Incorporated
InventorsGilbert De Angelis, Megan Aurora DeLamielleure, Guido Peters
Life of this patent
Estimating the term…
Abstract
A glass melt delivery system vessel has at least one sidewall and floor made of a refractory material, such as zirconia, and at least one electrode extending through the refractory material. The at least one electrode is configured to heat a glass melt in contact with the refractory material at an average temperature of at least about 1600 C° without exceeding a breakdown condition of the refractory material in contact with the glass melt.
Claims24
A glass melt delivery system vessel comprising:
- at least one sidewall and floor, wherein the at least one sidewall and floor comprise a refractory material;
- at least one electrode extending through the refractory material;
- wherein the at least one electrode is configured to heat a glass melt in contact with the refractory material at an average temperature of at least about 1600° C. without exceeding a breakdown condition of the refractory material in contact with the glass melt;
- wherein the melting vessel has a length and a width and the ratio of the length to the width ranges from about 2.4:1 to about 3.6:1 and wherein the melting vessel is configured to accept a glass melt having a depth of at least about 50% of the width of the melting vessel.
A method of making a glass article, the method comprising processing a glass composition in a glass melt delivery system vessel, the glass melt delivery system vessel comprising:
- at least one sidewall and floor, wherein the at least one sidewall and floor comprise a refractory material;
- at least one electrode extending through the refractory material;
- wherein the at least one electrode heats a glass melt in contact with the refractory material at an average temperature of at least about 1600° C. without exceeding a breakdown condition of the refractory material in contact with the glass melt;
- wherein the melting vessel comprises two opposing sidewalls, each opposing sidewall comprising at least two electrodes extending therethrough, wherein the ratio of the closest distance between the electrodes and a width of the electrodes in the lengthwise direction of the sidewall ranges from about 0.8:1 to about 2.4:1, and wherein a vertical distance between the floor and a bottom of one of the electrodes is at least about 5% of a length of the electrode in a vertical direction.
A glass article made by a method comprising processing a glass composition in a glass melt delivery system vessel, the glass melt delivery system vessel comprising:
- at least one sidewall and floor, wherein the at least one sidewall and floor comprise a refractory material;
- at least one electrode extending through the refractory material;
- wherein the at least one electrode heats a glass melt in contact with the refractory material at an average temperature of at least about 1600° C. without exceeding a breakdown condition of the refractory material in contact with the glass melt;
- wherein the melting vessel comprises the two opposing sidewalls, each opposing sidewall comprising at least two electrodes extending therethrough, wherein a ratio of the closest distance between the electrodes and a width of the electrodes in a lengthwise direction of the sidewall ranges from about 0.8:1 to about 2.4:1, and wherein a vertical distance between the floor and a bottom of the one of the electrodes is at least about 5% of a length of the electrode in the vertical direction.
An electronic device comprising a glass article made by a method comprising processing a glass composition in a glass melt delivery system vessel, the glass melt delivery system vessel comprising:
- at least one sidewall and floor, wherein the at least one sidewall and floor comprise a refractory material;
- at least one electrode extending through the refractory material;
- wherein the at least one electrode heats a glass melt in contact with the refractory material at an average temperature of at least about 1600° C. without exceeding a breakdown condition of the refractory material in contact with the glass melt:
- wherein the melting vessel comprises the two opposing sidewalls, each opposing sidewall comprising at least two electrodes extending therethrough, wherein a ratio of the closest distance between the electrodes and a width of the electrodes in a lengthwise direction of the sidewall ranges from about 0.8:1 to about 2.4:1, and wherein a vertical distance between the floor and a bottom of the one of the electrodes is at least about 5% of a length of the electrode in the vertical direction, wherein the glass article is the glass sheet.
Dependencies are inferred from the claim text.