Stable electrolyte matrix for molten carbonate fuel cells
AssigneeFuelCell Energy, Inc.
InventorsAbdelkader Hilmi, Arun Surendranath, Chao-Yi Yuh, Mohammad Farooque
Life of this patent
Estimating the term…
Abstract
A method of making an electrolyte matrix includes: preparing a slurry comprising a support material, a coarsening inhibitor, an electrolyte material, and a solvent; and drying the slurry to form an electrolyte matrix. The support material comprises lithium aluminate, the coarsening inhibitor comprises a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3, and mixtures thereof, and the coarsening inhibitor has a particle size of about 0.005 μm to about 0.5 μm.
Claims13
A method of making an electrolyte matrix comprising:
- preparing a slurry comprising:
- a support material comprising lithium aluminate,
- a coarsening inhibitor comprising a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3, and mixtures thereof, wherein the coarsening inhibitor has a particle size of about 0.005 μm to about 0.5 μm, and wherein the coarsening inhibitor has a BET surface area of about 10 m2/g to about 50 m2/g,
- an electrolyte material,
- a reinforcing material having an average particle size in a range of about 10 μm to about 120 μm, and
- a solvent;
- and
- drying the slurry to form an electrolyte matrix.
A method of making an electrolyte matrix comprising:
- forming a mixture of an aluminum containing precursor, a lithium containing precursor, and a dopant precursor, wherein the dopant precursor is in oxide or salt form;
- drying the mixture to form a powder;
- heat treating the powder at a temperature of about 550° C. to about 800° C. for a period of about 6 hours to about 30 hours to form a lithium aluminate including a dopant, wherein the dopant comprises a material selected from the group consisting of MnO2, Mn2O3, TiO2, ZrO2, Fe2O3, LiFe2O3 and mixtures thereof;
- preparing a slurry comprising the lithium aluminate including the dopant, an electrolyte material, and a solvent;
- and
- drying the slurry to form an electrolyte matrix.
Dependencies are inferred from the claim text.