Metal oxide particles and method of producing thereof
AssigneePhinergy Ltd.
InventorErnst Khasin
Life of this patent
Estimating the term…
Abstract
Methods of producing high purity powders of submicron particles of metal oxides are presented. The methods comprise providing or forming an alloy of a first metal with a second metal, optionally heating the alloy, subjecting the alloy to a leaching agent to remove the second metal from the alloy and to oxidize the first metal, thus forming submicron oxide particles of the first metal. Collections of high purity, high surface area, submicron particles are presented as well.
Claims19
Metal oxide clusters which comprise metal oxide particles at a size range between 3 nm and 200 nm,
- wherein the metal-oxide particles form a nano-porous structure and have a specific surface area that is larger than 70 m2/g,
- wherein the metal in said metal oxide particles includes Cu and Co, and
- wherein the crystalline structure of said metal oxide particles is perovskite, spinel or spinel-like.
Metal oxide clusters which comprise metal oxide particles at a size range between 3 nm and 200 nm, and have a rounded shape,
- wherein the metal-oxide particles form a nano-porous structure and have a specific surface area that is larger than 70 m2/g,
- wherein the metal(s) in said metal oxide particles comprise Ti, Fe, Zr, Hf, Cu, Co, Cr, Ni, Mo, La, Nb, Ta, W, V, or combinations thereof, and
- wherein the crystalline structure of said metal oxide particles is perovskite, spinel or spinel-like,
- wherein the metal oxide particles comprise titanium oxide particles.
A chemical catalyst in powder form comprising metal oxide clusters which comprise complex metal oxide particles at a size range between 3 nm and 200 nm, wherein the metal oxide clusters have a rounded shape, and form a nano-porous structure having a specific surface area larger than 70 m2/g,
- wherein the complex metal oxide particles comprise Ti,
- wherein the crystalline structure of said metal oxide particles is perovskite, spinel or spinel-like, and
- wherein a metal-base purity of said metal oxide particles is greater than 99%.
Dependencies are inferred from the claim text.