Method for producing a high strength steel sheet having improved strength and formability, and obtained high strength steel sheet
AssigneeArcelorMittal
InventorsPavan Venkatasurya, Hyun Jo Jun
Life of this patent
Estimating the term…
Loading patent…
AssigneeArcelorMittal
InventorsPavan Venkatasurya, Hyun Jo Jun
Estimating the term…
A method for producing a steel sheet having a microstructure including 71% to 91% martensite and bainite, 9% to 13% retained austenite, and at most 20% ferrite is provided. The method includes providing a cold-rolled steel sheet including, in weight percent: 0.13%≤C≤0.22%, 1.2%≤Si≤2.3%, 0.02%≤Al≤1.0%, with 1.25%≤Si+Al≤2.35%, 2.4%≤Mn≤3%, Ti≤0.05%, Nb≤0.05% and a remainder of Fe and unavoidable impurities, annealing the steel sheet to obtain 80% to 100% austenite and 0% to 20% ferrite, quenching the steel sheet at a cooling rate between 20° C./s and 50° C./s to a quenching temperature between 240° C. and 310° C., heating the steel sheet to a partitioning temperature between 400° C. and 465° C. and maintaining the steel sheet at the partitioning temperature for 50 to 250 seconds, then immediately cooling the sheet to room temperature. Steel sheets are also provided.
A method for producing an uncoated steel sheet having a microstructure consisting of, in surface percentage, between 71% and 91% of a sum of martensite and bainite, between 9% and 13% retained austenite, and at most 20% ferrite, the method comprising the following successive steps:
A method for producing an uncoated steel sheet having a microstructure consisting of, in surface percentage, between 71% and 91% of a sum of martensite and bainite, between 9% and 13% retained austenite, and at most 20% ferrite, wherein the method comprises the following successive steps:
An uncoated steel sheet, wherein the uncoated steel sheet is made of a steel having a chemical composition containing by weight:
A steel sheet wherein the steel sheet is made of a steel having a chemical composition containing by weight:
Dependencies are inferred from the claim text.