Formed hexagonal boron nitride body, heat-treated hexagonal boron nitride body and processes for producing the same
Assignee3M Innovative Properties Company
InventorsJan C. Zimmer, Ursula Kayser, Krishna B. Uibel, Christoph Lesniak
Life of this patent
Estimating the term…
Abstract
Provided are materials for a formed body comprising hexagonal boron nitride and such formed bodies. Also provided are heat-treated formed body obtained by heat-treating the formed bodies. The invention further relates to processes for making the formed body and the heat-treated formed body.
Claims13
A formed body comprising a material composition, the material composition comprising hexagonal boron nitride, a water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, and boehmite, wherein as expressed as a molar ratio of AlO(OH):
- H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1, wherein the boehmite is able to split off a gaseous phase at a heat treatment at a temperature of at most 1000° C., and is able to form, with the water-soluble boron compound, a water-insoluble boron compound at a heat treatment at a temperature of 200-1000° C.;
- wherein the gaseous phase is water, carbon dioxide, or a combination thereof.
A process of making a formed body, wherein the process comprises the steps
- (a) providing a first powder comprising hexagonal boron nitride powder;
- (b) obtaining a second powder comprising the hexagonal boron nitride powder and at least one water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, by at least one of:
- (i) generating the at least one water soluble boron compound by mechanically pre-treating the powder of step (a) and
- (ii) by adding the at least one water-soluble boron compound to the powder provided in step (a);
- (c) adding boehmite to the second powder of step (b), wherein as expressed as a molar ratio of AlO(OH):
- H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1 ;
- (d) mixing the second powder of step (b) and the boehmite added in step (c), thereby obtaining a material composition comprising hexagonal boron nitride;
- (e) optionally granulating the material composition of step (d), thereby obtaining a material composition comprising hexagonal boron nitride, wherein the material composition is granulated;
- and
- (f) forming the material composition of step (d) or the material composition of step (e) into a shape.
A process for making a heat-treated formed body, wherein the process comprises the steps
- (a) providing a first powder comprising hexagonal boron nitride powder;
- (b) obtaining a second powder comprising hexagonal boron nitride powder and at least one water-soluble boron compound selected from the group consisting of boric acid (H3BO3) and ammonium borates, by at least one of:
- (i)generating the at least one water soluble boron compound by mechanically pre-treating the first powder of step (a) and
- (ii) by adding the at least one water-soluble boron compound to the first powder provided in step (a), thereby;
- (c) adding boehmite to the second powder of step (b), wherein as expressed as a molar ratio of AlO(OH):
- H3BO3, the molar ratio of boehmite to the water-soluble boron compound is from 0.3:1 to 6:1 the further inorganic compound;
- (d) mixing the second powder of step (b) and the boehmite added in step (c), thereby obtaining a material composition comprising hexagonal boron nitride;
- (e) optionally granulating the material composition of step (d), thereby obtaining a material composition comprising hexagonal boron nitride, wherein the material composition is granulated;
- and
- (f) forming the material composition of step (d) or the material composition of step (e) into a shape, thereby obtaining a formed body;
- and
- (g) heat-treating the formed body of step (f) at a temperature of from 200 to 1000° C.