Strengthened thin glass-polymer laminates
AssigneeCorning Incorporated
InventorsKiat Chyai Kang, Govindarajan Natarajan, Yu Xiao
Life of this patent
Estimating the term…
Abstract
A glass-polymer laminate structure includes a flexible glass substrate having a thickness of no more than about 0.3 mm. A polymer layer is laminated to a surface of the flexible glass substrate having a coefficient of thermal expansion (CTE) that is at least about 2 times a CTE of the flexible glass substrate. The polymer layer is laminated to the surface of the flexible glass substrate after thermally expanding the polymer layer to provide the flexible glass substrate with an in-plane compressive stress of at least about 30 MPa along a thickness of the flexible glass substrate.
Claims19
A thermally bent, asymmetric glass-polymer laminate structure comprising:
- a flexible glass substrate having a thickness of no more than about 0.3 mm;
- a polymer layer laminated to a first surface of the flexible glass substrate, and
- an adhesive layer that laminates the polymer layer to the flexible glass substrate wherein the polymer layer has a coefficient of thermal expansion (CTE) that is at least 2 times a CTE of the flexible glass substrate, or has a CTE that is at least 3 ppm/° C. greater than a CTE of the flexible glass substrate,
- and wherein the polymer layer is laminated to the first surface of the flexible glass substrate using the adhesive that sets only after thermally expanding the polymer layer at an elevated temperature of greater than 20° C. and less than the softening temperature of the polymer to bond the polymer layer to the flexible glass substrate while thermally expanded to provide the flexible glass substrate with a thermally bent configuration that is bent toward the polymer layer when the polymer layer is controllably cooled at a rate of less than or equal to 1-2° C./minute thereby reducing a tensile stress in the flexible glass substrate due to the bent configuration;
- wherein the flexible glass substrate has a compressive stress of greater than about 30 MPa at the first surface and a tensile stress of less than about 40 MPa at a second surface that is opposite the first surface.
Dependencies are inferred from the claim text.