A method for manufacturing a skateboard, specifically comprising steps of:
- step (1) manufacturing an internal core board, comprising:
- foaming an organic polymer material with steam with a temperature at a range of 160-180° C. to produce a foam board as the internal core board;
- step (2) manufacturing an upper surface board and a lower surface board, comprising:
- sending the organic polymer material into an oven for heating to 190-210° C. to perform foam molding for serving as a foam
- step (3) cutting and molding, comprising:
- cutting the foam board in the step (1) into an internal core layer 1 which is preset in step 4;
- step (4) manufacturing a plate body, comprising:
- placing the internal core layer (1) between the upper surface layer (2) and the lower surface layer (3), and then adhering the upper surface layer (2) and the lower surface layer (3) with the internal core layer (1) together by EVA resin, and wrapping the internal core layer (1) between the upper surface layer (2) and the lower surface layer (3) to form a board according to requirement of a skateboard;
- step (5) manufacturing a pattern layer on a surface of the plate body, comprising:
- printing a pattern layer (5) on a surface of the plate body by laser printing;
- and
- step (6) manufacturing a plastic film, and a layer of plastic film (4) is cast on the pattern layer on the bottom surface of the plate body, casting a layer of the plastic film (4) on the pattern layer provided on a bottom layer of the plate body, in such a manner that the method for manufacturing the skateboard is completed;
- wherein a process of the laser printing comprises steps of:
- step (a) performing primer treatment on a PET film with an acrylic resin, and performing laser embossing on the PET film treated, and then vacuum-aluminizing the PET film to obtain a composite PET film desired;
- step (b) covering a composite PET film with polyurethane printing ink by gravure to form an ink layer, and painting a surface of the ink layer printed with an acrylic resin by a brush to form a protective film layer;
- step (c) brushing polyurethane glue on a surface of the PE film which is transparent, after drying in an oven, covering a glue surface of the PE film on an ink surface of the composite PET film, and then pressing by a press roll, wherein a pressing pressure is at a range of 0.8-1.2 MPa, a temperature of a pressure roller is at a range of 60-80° C.;
- after the pressing, the PET film is peeled off the PE film to transfer an ink and laser effect to the PE film which is transparent;
- step (d) brushing a layer of polyurethane glue on an external surface of a porcelain white PE film, then sending porcelain white PE film with the layer of polyurethane glue brushed into the oven for drying, and then covering and adhering a glue surface of the porcelain white PE film dried on an the ink surface of the PE film which is transparent;
- step (e) transferring the PE film adhered to a curing chamber at a constant temperature of 40° C. for aging, and taking out after an aging time of 46-50 hours to obtain a laser PE film;
- step (f) coating and adhering a porcelain white PE film surface of the laser PE film on an external surface of the plate body by glue coating, thereby obtaining a laser printing pattern.