Method, process and fabrication technology for oxide layers
AssigneeSpecmat Limited
InventorsHoria M. Faur, Maria Faur
Life of this patent
Estimating the term…
Abstract
This disclosure relates to a Room Temperature Wet Chemical Growth (RTWCG) method and process of SiOX thin film coatings which can be grown on various substrates. The invention further relates to RTWCG method and process suited to grow thin films on the Si substrates used in the manufacture of silicon-based electronic and photonic (optoelectronic) device applications. The invention further relates to processes used to produce SiOX thin film layers for use as passivation layers, low reflectance layers, or high reflectance single layer coatings (SLARC) and selective emitters (SE).
Claims7
A method for growing, or creating, a passivation oxide on silicon, the method comprising the steps of:
- (A) supplying a chemical solution comprising:
- (A1) one or more fluorine-containing acid compounds or fluorine-containing acids, wherein the one or more fluorine-containing acid compounds or fluorine-containing acids are present in the range of about 35% by weight to about 50% by weight;
- (A2) nitric acid, wherein the nitric acid is present in the range of about 0.00224% by weight to about 1.32% by weight;
- (A3) one or more of 2,4-dihydroxypyridine, pyridine, dichloropyridazin-3(2H)-one and/or pyridoxine hydrochloride, wherein the one or more of 2,4-dihydroxypyridine, pyridine, dichloropyridazin-3(2H)-one and/or pyridoxine hydrochloride are present in the range of about 0.005% by weight to about 25% by weight;
- (A4) optionally, one or more additional compounds selected from:
- (A4a) one or more iodine-containing acids, wherein the one or more iodine-containing acids are present in the range of about 0.00005% by weight to about 0.25% by weight;
- and/or
- (A4b) one or more selenium-containing acid compounds or selenium-containing acids, wherein the one or more selenium-containing acid compounds or selenium-containing acids, when present, are present in the range of about 0.00005% by weight to about 0.25% by weight;
- and
- (A5) the remainder of the chemical solution being water;
- (B) exposing a silicon surface to the solution of Step (A);
- and
- (C) subjecting the silicon to a thermal treatment step comprising:
- (C1) a ramp-up step of about 400 seconds at a temperature of from about 350° C. to about 725° C.;
- (C2) a plateau step of about 300 seconds;
- and
- (C3) a ramp down step to room temperature,
- wherein the solution is formulated to grow a thin oxide film that passivates the surface after the thermal treatment of Step (C) has been applied thereto.