This present invention relates to a Room Temperature Wet Chemical Growth (RTWCG) formulations, methods and processes. In one embodiment, the present invention further relates to RTWCG formulations, methods and processes that utilize a low-[HF]. In another embodiment, the present invention relates to RTWCG formulations with improved bath life.
Claims14
A composition and/or formulation for room temperature wet chemical growth (RTWCG) of an oxide film, or layer, the composition and/or formulation comprising:
- from about 0.01 percent by weight to about 0.4 percent by weight of Component A, where Component A is selected from one or more iodine-containing compounds;
- (ii) from about 0.1 percent by weight to about 8.2 percent by weight of Component B, where Component B is selected from one or more of HF or NH4F;
- (iii) from about 13 percent by weight to about 37 percent by weight of Component C, where Component C is selected from one or more non-oxidizing acids of HCl or HBr;
- and
- (iv) from about 0.01 percent by weight to about 10 percent by weight of Component D, where Component D is selected from one or more pyridine compounds, wherein the one or more pyridine compounds contain at least one —OH substituent group,
- wherein the remaining percent by weight of the composition and/or formulation containing Components A, B, C and D is water so as to yield a 100 percent by weight composition and/or formulation, and
- wherein the composition and/or formulation achieves the growth of a SiOX film, or layer, on a silicon substrate.
A composition and/or formulation for room temperature wet chemical growth (RTWCG) of an oxide film, or layer, containing a low concentration of HF, the composition and/or formulation comprising:
- (a) from about 0.01 percent by weight to about 0.4 percent by weight of Component A, where Component A is HIO3;
- (b) from about 3.2 percent by weight to about 8.2 percent by weight of Component B, where Component B is HF;
- (c) from about 13 percent by weight to about 37 percent by weight of Component C, where Component C is selected from one or more non-oxidizing acids of HCl or HBr;
- and
- (d) from about 0.01 percent by weight to about 2.2 percent by weight of Component D, where Component D is 2,4-dihydroxypyridine,
- wherein the remaining percent by weight of the composition and/or formulation containing Components A, B, C and D is water so as to yield a 100 percent by weight composition and/or formulation, and
- wherein the composition and/or formulation achieves the growth of a SiOX film, or layer, on a silicon substrate.
A composition and/or formulation for room temperature wet chemical growth (RTWCG) of a passivation film, or layer, containing a low concentration of HF, the composition and/or formulation comprising:
- from about 0.01 percent by weight to about 0.4 percent by weight of Component A, where Component A is HIO3;
- from about 3.2 percent by weight to about 8.2 percent by weight of Component B, where Component B is HF;
- from about 13 percent by weight to about 37 percent by weight of Component C, where Component C is HCl;
- and
- from about 0.01 percent by weight to about 2.2 percent by weight of Component D, where Component D is 2,4-dihydroxypyridine,
- wherein the remaining percent by weight of the composition and/or formulation containing Components A, B, C and D is water so as to yield a 100 percent by weight composition and/or formulation, and
- wherein the composition and/or formulation achieves the growth of a SiOX-based passivation oxide film, or layer, on a silicon substrate.
Dependencies are inferred from the claim text.