Method of manufacturing electrode slurry for lithium secondary battery, and electrode slurry
AssigneeFdk Corporation
InventorsYuki Ochiai, Keita Yamamoto
Life of this patent
Estimating the term…
Loading patent…
AssigneeFdk Corporation
InventorsYuki Ochiai, Keita Yamamoto
Estimating the term…
Slurry is prepared by dispersing a solvent containing fibrous carbon (carbon nanotube, vapor grown carbon fiber (VGCF (registered trademark))) by using a media-type disperser, and the slurry to be applied to a collector is obtained by kneading the prepared slurry and an electrode active material. As a media-type disperser, for example, a ball mill disperser or a bead mill disperser is used. The dispersion using the media-type disperser is performed for 5 to 10 hours. As a dispersant, for example, at least any one of a nonionic dispersant, an ethylenic dispersant, a polymeric dispersant and an amine dispersant is used. The dispersion is performed so that a fiber length of the fibrous carbon becomes 2 to 7 μm.
A method of manufacturing electrode slurry for a lithium secondary battery, the method comprising:
Dependencies are inferred from the claim text.