# US H2,104 H1 · Polyolefin foam/film composite and method for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US H2,104 H1
- Document ID: USH2104H1
- Status: Granted
- Kind: H1
- Application number: 09/605,499
- Filed: 2000-06-28
- Granted: 2004-05-04
- Earliest claimed: 2000-06-28
- Assignees: Sealed Air Corporation (US)
- Inventors: Natarajan S. Ramesh
- Web page: https://patentgrep.com/patent/USH2104H1

## Abstract

A composite structure, which includes: a. a foam sheet comprising polyolefin; and b. a film sheet adhered to the foam sheet, wherein the film sheet (1) comprises polypropylene, (2) is stretch-oriented in at least one direction, (3) has a thickness of less than 0.9 mil, and (4) has a larger surface area than the foam sheet such that at least one edge of the film sheet extends beyond a corresponding edge of the foam sheet.

## Claims

### Claim 1

A composite structure, comprising:
a. a foam sheet comprising polyolefin; and
b. a film sheet adhered to said foam sheet, wherein said film sheet
(1) comprises polypropylene,
(2) is stretch-oriented in at least one direction,
(3) has a thickness of less than 0.9 mil, and
(4) has a larger surface area than said foam sheet such that at least one edge of said film sheet extends beyond a corresponding edge of said foam sheet.

### Claim 2 (depends on 1)

The composite structure of claim 1, wherein said polyolefin foam sheet comprises polyethylene homopolymer or copolymer.

### Claim 3 (depends on 2)

The composite structure of claim 2, wherein said polyolefin foam sheet has a density ranging from about 1 to about 10 pounds/ft3 and a thickness ranging from about 0.004 to about 2 inches.

### Claim 4 (depends on 1)

The composite structure of claim 1, wherein said film sheet is stretch-oriented in at least two directions.

### Claim 5 (depends on 4)

The composite structure of claim 4, wherein said film sheet has an orientation ratio of at least 2 in both of said at least two directions.

### Claim 6 (depends on 1)

The composite structure of claim 1, wherein said film has a thickness 0.6 mil or less.

### Claim 7 (depends on 1)

The composite structure of claim 1, wherein said film includes at least a first layer comprising said polypropylene and a second layer interposed between and bonding said film and foam sheets.

### Claim 8 (depends on 7)

The composite structure of claim 7, wherein said foam sheet and film sheet are adhered via heat lamination.

### Claim 9 (depends on 1)

The composite structure of claim 1, wherein said composite structure has a maximum water vapor transmission rate of 0.6 grams/100 in2 per 24 hours @ 100° F. and 90% relative humidity.

### Claim 10 (depends on 9)

The composite structure of claim 9, wherein said composite structure has a maximum water vapor transmission rate of 0.5 grams/100 in2 per 24 hours @ 100° F. and 90% relative humidity.

### Claim 11

A method for making a composite structure, comprising:
a. providing a foam sheet comprising polyolefin; and
b. providing a film sheet and adhering said film sheet to said foam sheet, wherein said film sheet
(1) comprises polypropylene,
(2) is stretch-oriented in at least one direction,
(3) has a thickness of less than 0.9 mil, and
(4) has a larger surface area than said foam sheet such that at least one edge of said film sheet extends beyond a corresponding edge of said foam sheet.

### Claim 12 (depends on 11)

The method of claim 11, wherein said polyolefin foam sheet comprises polyethylene homopolymer or copolymer.

### Claim 13 (depends on 12)

The method of claim 12, wherein said polyolefin foam sheet has a density ranging from about 1 to about 10 pounds/ft3 and a thickness ranging from about 0.004 to about 2 inches.

### Claim 14 (depends on 11)

The method of claim 11, wherein said film sheet is stretch-oriented in at least two directions.

### Claim 15 (depends on 14)

The method of claim 14, wherein said film sheet has an orientation ratio of at least 2 in both of said at least two directions.

### Claim 16 (depends on 11)

The method of claim 11, wherein said film has a thickness 0.6 mil or less.

### Claim 17 (depends on 11)

The method of claim 11, wherein said film includes at least a first layer comprising said polypropylene and a second layer interposed between and bonding said film and foam sheets.

### Claim 18 (depends on 17)

The method of claim 17, wherein said foam sheet and film sheet are adhered via heat lamination.

### Claim 19 (depends on 11)

The method of claim 11, wherein said composite structure has a maximum water vapor transmission rate of 0.6 grams/100 in2 per 24 hours @ 100° F. and 90% relative humidity.

### Claim 20 (depends on 19)

The method of claim 19, wherein said composite structure has a maximum water vapor transmission rate of 0.5 grams/100 in2 per 24 hours @ 100° F. and 90% relative humidity.