# US 9,994,937 B1 · Mo-Si-B manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,994,937 B1
- Document ID: US9994937B1
- Status: Granted
- Kind: B1
- Application number: 14/717,603
- Filed: 2015-05-20
- Granted: 2018-06-12
- Earliest claimed: 2014-05-20
- Assignees: Imaging Systems Technology
- Applicants: Carol Ann Wedding; Joe K. Cochran; Oliver M. Strbik, III; Peter E. Marshall
- Inventors: Carol Ann Wedding; Joe K. Cochran; Oliver M. Strbik, III; Peter E. Marshall
- Web page: https://patentgrep.com/patent/US9994937B1

## CPC

- C22C 1/057: with in situ formation of phases other than hard compounds by solid state reaction sintering, e.g. metal phase formed by reduction reaction
- B22F 9/026: {Spray drying of solutions or suspensions}
- C22C 1/045: {Alloys based on refractory metals}
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method for controlling the formation of molybdenum solid solution in Mo—Si—B composites which comprises processing at 1400° C. or less to minimize, if not prevent, the silicon from going into solid solution in the molybdenum.

## Claims

### Claim 1

The process of forming a molybdenum silicon boron composite which includes the steps of:
combining precursor powders and heating to form Mo—Si—B;
forming a slurry of precursor powders and liquid;
spray drying the slurry to form a homogenous powder mixture;
sintering the homogenous powder in a reducing atmosphere;
compacting the powder; and
sintering the compacted powder.

### Claim 2 (depends on 1)

The process of claim 1 in which the precursor powders include molybdenum, silicon nitride, and boron nitride.

### Claim 3 (depends on 1)

The process of claim 1 in which the slurry is ball milled prior to spraying.

### Claim 4 (depends on 1)

The process of claim 1 in which spray drying parameters of drying temperature and slurry feed rate are controlled to achieve a powder particle size below 100 microns.

### Claim 5 (depends on 4)

The process of claim 4 in which the spray drying parameters of drying temperature and feed rate are controlled to achieve a powder particle size between 10 to 60 microns.

### Claim 6 (depends on 1)

The process of claim 1 in which teh sintering of the homogeneous powder is at a temperature below 1400° C.

### Claim 7 (depends on 1)

The process of claim 1 in which the sintering of the homogeneous powder is at a temperature below 1350° C.

### Claim 8 (depends on 1)

The process of claim 1 in which the sintering of the homogeneous powder is at a temperature below 1300° C.

### Claim 9 (depends on 1)

The process of claim 1 in which the reducing atmosphere is hydrogen.

### Claim 10 (depends on 1)

The process of claim 1 in which the reducing atmosphere is carbon monoxide.

### Claim 11 (depends on 1)

The process of claim 1 in which the sintened compacted powder is stored under vacuum.

### Claim 12 (depends on 1)

The process of claim 1 in which the powder is milled prior to compacting.

### Claim 13 (depends on 1)

The process of claim 1 in which the compacting and sintering are conducted in a reduced oxygen atmosphere.

### Claim 14 (depends on 1)

The process of claim 1 in which the compacting is achieved through cold isostatic pressing at a pressure above 10,000 psi.

### Claim 15 (depends on 1)

The process of claim 1 in which the sintering of the compacted powder is conducted at a temperature below 1400° C.

### Claim 16 (depends on 1)

The process of claim 1 in which the sintering of the compacted powder is conducted at a temperature below 1300° C.

### Claim 17 (depends on 1)

The process of claim 1 in which the sintering of the compacted powder is conducted under a pressure greater than 10,000 psi.

### Claim 18 (depends on 1)

The process of claim 1 in which the sintering of the compacted powder is conducted under a pressure greater than 50,000 psi.