Functional ecostone and method for manufacturing same
AssigneeIneco Inc.
InventorJae Moo Shin
Life of this patent
Estimating the term…
Abstract
Disclosed are a functional Ecostone and a method for manufacturing the same, wherein the functional Ecostone is characterized in that, on the basis of 100 parts by weight of a raw material formed by mixing 30-60 wt % of gypsum, 20-40 wt % of calcium carbonate, and 10-30 wt % of water, 1-30 parts by weight of a rose geranium extract, 2-10 parts by weight of basalt fibers, 2-10 parts by weight of mulberry fibers, 1-30 parts by weight of phytoncide, 1-30 parts by weight of ocher, and 1-30 parts by weight of charcoal are mixed.
Claims3
A molded functional ecostone for building materials, the functional ecostone comprising:
- 1 to 30 parts by weight of a rose geranium extract, 2 to 10 parts by weight of basalt fibers, 2 to 10 parts by weight of mulberry fibers, 1 to 30 parts by weight of phytoncide, 1 to 30 parts by weight of ocher, and 1 to 30 parts by weight of charcoal, on a basis of 100 parts by weight of a raw material formed by mixing 30 to 60 wt % of gypsum, 20 to 40 wt % of calcium carbonate, and 10 to 30 wt % of water.
A method for manufacturing a functional ecostone, the method comprising:
- forming a raw material by mixing 30 to 60 wt % of gypsum, 20 to 40 wt % of calcium carbonate, and 10 to 30 wt % of water;
- forming a mixture by mixing 1 to 30 parts by weight of a rose geranium extract, 2 to 10 parts by weight of basalt fibers, 2 to 10 parts by weight of mulberry fibers, 1 to 30 parts by weight of phytoncide, 1 to 30 parts by weight of ocher, and 1 to 30 parts by weight of charcoal on a basis of 100 parts by weight of the raw material;
- and
- injecting the mixture into a molding frame or a mold and then demolding the mixture.
Dependencies are inferred from the claim text.