Farnesene-based polymers and liquid optically clear adhesive compositions incorporating the same
AssigneeFina Technology, Inc.
InventorsTaejun Yoo, Herbert Chao, Steven K. Henning
Life of this patent
Estimating the term…
Loading patent…
AssigneeFina Technology, Inc.
InventorsTaejun Yoo, Herbert Chao, Steven K. Henning
Estimating the term…
A low viscosity polymer having a linear or branched backbone derived from farnesene monomers and at least one terminal-end functionalized with a hydroxyl group. This polymer may be further hydrogenated to reduce unsaturation and acrylated, such that it may be incorporated into a LOCA composition. The LOCA composition may be used in a laminated screen assembly, such as a touch screen, for electronic devices by adhering the LOCA composition between an optically transparent layer, such as a cover glass, and a display. The cured LOCA composition has a refractive index similar to the optically transparent layer. A method of making the low viscosity polymer for the LOCA composition includes anionically polymerizing farnesene monomers, quenching a living end of the polymer to provide the hydroxyl-terminated polymer; hydrogenating the hydroxyl-terminated polymer; and reacting the at least partially saturated hydroxyl-terminated polymer with at least one reagent to provide an acrylate terminated hydrogenated polymer.
A liquid optically clear adhesive composition comprising a polymer derived from monomers comprising farnesene, the polymer being obtained from a diol wherein hydroxyl groups of the diol have been further reacted to provide terminal ends functionalized with (meth)acrylate groups and wherein the polymer has a degree of unsaturation of less than or equal to 50%, wherein the adhesive composition has a refractive index greater than 1.45 after curing.
A method of preparing a liquid optically clear adhesive composition comprising:
A polymer comprising a linear or branched backbone derived from a monomer feed comprising farnesene and a comonomer, the farnesene content of the monomer feed being greater than or equal to 25%, by mole, the polymer having terminal ends functionalized with (meth)acrylate groups and a viscosity at 60° C. of equal to or less than 25,000 cP before curing.
Dependencies are inferred from the claim text.