US 9,849,532 B2Granted
Composite wear pad and methods of making the same
AssigneeKennametal Inc.
InventorsQingjun Zheng, Robert J. Vasinko, Yixiong Liu
Life of this patent
Estimating the term…
Abstract
A composite wear pad includes a substrate that is selected from the group of iron based alloys, steel, nickel based alloys, and cobalt based alloys. A hard particle-matrix alloy layer is bonded at a surface to the substrate. The hard particle-matrix alloy layer has a plurality of hard particles dispersed in a matrix alloy. The hard particle-matrix alloy layer has a thickness ranging between greater than about 13 millimeters and about 20 millimeters.
Claims20
A composite wear pad comprising:
- a substrate being selected from the group consisting of iron based alloys, steel, nickel based alloys, and cobalt based alloys, the substrate comprising a surface for engaging an article;
- a hard particle-matrix alloy layer bonded metallurgically to the substrate, the hard particle-matrix alloy layer comprising a plurality of hard particles dispersed uniformly in a nickel-based matrix alloy;
- and
- the hard particle-matrix alloy layer of the composite wear pad having a thickness ranging between greater than about 13 millimeters and about 20 millimeters, wherein the hard particle-matrix alloy layer is void-free.
1 more element