Back to results
US 9,809,695 B2Granted
Poly(vinyl acetal) resin compositions, layers, and interlayers having enhanced optical properties
AssigneeSolutia Inc.
InventorsJun Lu, Zhou Li
Life of this patent
Estimating the term…
Abstract
Resin compositions, layers, and interlayers comprising two or more thermoplastic polymers and at least one RI balancing agent for adjusting the refractive index of at least one of the resins or layers is provided. Such compositions, layers, and interlayers exhibit enhanced optical properties while retaining other properties, such as impact resistance and acoustic performance.
Claims12
An interlayer comprising:
- a first poly(vinyl acetal) resin;
- a second poly(vinyl acetal) resin having a residual hydroxyl content that is at least 2 weight percent higher or lower than the residual hydroxyl content of said first poly(vinyl acetal) resin;
- at least one plasticizer, wherein each plasticizer present in said interlayer has a refractive index of less than 1.460;
- and
- a refractive index (RI) balancing agent, wherein said RI balancing agent includes residues of a high RI aldehyde, and wherein said first poly(vinyl acetal) resin comprises at least 0.5 weight percent of said residues of said high RI aldehyde, based on the total weight of aldehyde residues of said first poly(vinyl acetal) resin,
- wherein each of said first and second poly(vinyl acetal) resin are present in said interlayer in an amount of at least 0.5 weight percent, based on the total weight of resins in said interlayer, and wherein said interlayer has a haze value of not more than 5 percent, and
- wherein said interlayer comprises a multilayer interlayer having at least a first resin layer and a second resin layer adjacent to said first resin layer, wherein said first resin layer comprises said first poly(vinyl acetal) resin and said second resin layer comprises said second poly(vinyl acetal) resin, wherein said RI balancing agent is present in at least one of said first and said second resin layers, and wherein the absolute value of the difference between the refractive index of said first resin layer and the refractive index of said second resin layer is not more than 0.010.
4 more elements
The, An interlayer comprising:
- a first poly(vinyl acetal) resin;
- a second poly(vinyl acetal) resin having a residual hydroxyl content that is at least 2 weight percent higher or lower than the residual hydroxyl content of said first poly(vinyl acetal) resin;
- at least one plasticizer, wherein each plasticizer present in said interlayer has a refractive index of less than 1.460;
- and
- a refractive index (RI) balancing agent, wherein said RI balancing agent comprises residues of a high RI aldehyde, wherein said first poly(vinyl acetal) resin comprises at least 0.5 weight percent of residues of said high RI aldehyde, based on the total weight of aldehyde residues of said first poly(vinyl acetal) resin,
- wherein each of said first and second poly(vinyl acetal) resin are present in said interlayer in an amount of at least 0.5 weight percent, based on the total weight of resins in said interlayer, and wherein said interlayer has a haze value of not more than 5 percent,
- wherein said interlayer comprises a blended resin that includes said first and said second poly(vinyl acetal) resins, wherein one of said first and said second poly(vinyl acetal) resins is dispersed within the other of said first and said second poly(vinyl acetal) resins thereby forming domains of said one of said first and said second poly(vinyl acetal) resins within said other of said first and said second poly(vinyl acetal) resins, and wherein, when blended, the absolute value of the difference between the refractive index of said first poly(vinyl acetal) resin domains and the refractive index of said second poly(vinyl acetal) resin domains is not more than 0.010.
4 more elements
An interlayer comprising:
- a first poly(vinyl acetal) resin;
- a second poly(vinyl acetal) resin;
- and
- a refractive index (RI) balancing agent, wherein said RI balancing agent includes residues of a high RI aldehyde present in at least one of said first and said second poly(vinyl acetal) resins,
- wherein said high RI aldehyde is present in an amount of at least 0.5 weight percent, based on the total weight of aldehyde residues of said first or said second poly(vinyl acetal) resin,
- wherein said interlayer has a haze value of not more than 5 percent and a loss factor at 20° C. of at least 0.10, and
- wherein, in the absence of said RI balancing agent, said interlayer has a haze value of at least 5 percent.
4 more elements