Method for producing a steel tube including cleaning of the outer tube wall
AssigneeSandvik Materials Technology Deutschland GmbH
InventorsThomas Frobose, Udo Rauffmann
Life of this patent
Estimating the term…
Abstract
A method for producing a steel tube include the manufacturing of a steel tube having an inner tube wall, an outer tube wall (3), and a free tube cross-section enclosed by the inner tube wall. After the manufacturing, the steel tube includes at least one contaminant on the outer tube wall and entails, after the manufacturing of the steel tube, cleaning of the outer tube wall by applying liquid or solid CO2 onto the outer tube wall in order to remove a contaminant from the outer tube wall.
Claims13
A method for producing a steel tube comprising:
- manufacturing the steel tube by forming a hollow shell into a form of a finished dimensioned steel tube by cold pilgering, the steel tube having an inner tube wall, an outer tube wall, and a free tube cross-section enclosed by the inner tube wall, wherein after the manufacturing, the steel tube on the outer tube wall includes at least one contaminant, the at least one contaminant being a lubricant transferred from a roll to the outer tube wall;
- and
- cleaning the outer tube wall of the steel tube by applying liquid or solid CO2 onto the outer tube wall in order to remove the lubricant from the outer tube wall,
- wherein, during the application of the liquid or solid CO2 onto the outer tube wall, the temperature of the steel tube is measured and the cleaning is interrupted if the temperature of the steel tube falls below a predetermined temperature threshold.
A method for producing a steel tube comprising:
- manufacturing the steel tube by forming a hollow shell into a form of a finished dimensioned steel tube by cold drawing the hollow shell into the form of the finished steel tube, the steel tube having an inner tube wall, an outer tube wall, and a free tube cross-section enclosed by the inner tube wall, wherein after the manufacturing, the steel tube on the outer tube wall includes at least one contaminant, the at least one contaminant being a drawing oil transferred from a die to the outer tube wall;
- cleaning the outer tube wall by applying liquid or solid CO2 onto the outer tube wall in order to remove the drawing oil from the outer tube wall;
- measuring a temperature of the steel tube during cleaning;
- and
- interrupting the cleaning when the measured temperature of the steel tube is below a predetermined temperature threshold.
A method for producing a steel tube comprising:
- manufacturing the steel tube by forming a hollow shell into a form of a finished dimensioned steel tube by cold pilgering, the steel tube having an inner tube wall, an outer tube wall, and a free tube cross-section enclosed by the inner tube wall, wherein after the manufacturing, the steel tube on the outer tube wall includes at least one contaminant, the at least one contaminant being a lubricant transferred from a roll to the outer tube wall;
- and
- cleaning the outer tube wall of the steel tube by applying liquid or solid CO2 onto the outer tube wall in order to remove the lubricant from the outer tube wall;
- wherein the liquid or solid CO2 is applied in the form of a jet onto the outer tube wall, wherein a jet direction of the CO2 is substantially perpendicular to the outer tube wall.,
- wherein a temperature of the jet is measured in the jet direction of the liquid or solid CO2 after the liquid or solid CO2 has interacted with the outer tube wall of the steel tube, and
- wherein a velocity of the liquid or solid CO2 as it exits a feed line is regulated as a function of the temperature of the jet in the jet direction of the liquid or solid CO2 after the liquid or solid CO2 has interacted with the outer tube wall of the steel tube.
Dependencies are inferred from the claim text.