Physically modified extracellular matrix materials and uses thereof
AssigneeCook Biotech Incorporated
InventorsChad E. Johnson, David M. J. Ernst, Michael Hiles, F. Joseph Obermiller
Life of this patent
Estimating the term…
Abstract
Described are expanded collagenous materials and methods for their preparation and use. Certain expanded collagenous materials can be prepared by treating a first collagenous material with an alkaline substance under conditions effective to expand the first collagenous material, and recovering the expanded material. Expanded materials can exhibit beneficial persistence and tissue generation characteristics when implanted, and can be used in the formation of highly porous medical implant bodies which can be compressed to fractions of their original volume and will thereafter substantially recover their original volume.
Claims16
A method for preparing a compressible graft construct, comprising:
- contacting a first extracellular matrix material with an alkaline aqueous liquid having a pH between 8 and 14 to form a second, expanded extracellular matrix material, said first extracellular matrix material comprising at least 80% by weight collagen on a dry weight basis, wherein said contacting is sufficient to denature collagen of the first extracellular matrix material such that denatured collagen is present in the second expanded extracellular matrix material, wherein said second expanded extracellular matrix material has a volume of at least 120% that of the volume of said first extracellular matrix material, and wherein said first extracellular matrix material is a sheet material, and wherein upon completion of said contacting, the expanded extracellular matrix material is a sheet material;
- charging the expanded extracellular matrix material to a mold;
- and
- drying the expanded extracellular matrix material to form the compressible graft construct.
A method for preparing an implantable plug graft, comprising:
- contacting a first extracellular matrix material with an alkaline aqueous liquid having a pH between 8 and 14 to form a second, expanded extracellular matrix material, wherein said contacting is sufficient to denature collagen of the first extracellular matrix material such that denatured collagen is present in the second expanded extracellular matrix material, wherein said second expanded extracellular matrix material has a volume of at least 120% that of the volume of said first extracellular matrix material;
- and wherein said first extracellular matrix material is a sheet material, and wherein upon completion of said contacting, the expanded extracellular matrix material is a sheet material;
- and
- preparing a plug comprising the expanded extracellular matrix material.