A density controlled cold fusion concrete cementitious spray applied fireproofing material including a mixture of water, one or more of silicon dioxide, expanded glass, vermiculite, bottom ash, perlite, expanded shale, or other lightweight aggregates of various diameter sizes ranging from about 0.025 mm to about 12.5 mm in diameter; anhydrous or hydrous sodium or potassium metasilicate; waste from steel production consisting of Granulated Ground Blast Furnace Slag (GGBFS); high calcium or low calcium waste from coal combustion (fly ash or bottom ash); sodium tetraborate, sodium citrate dihydrate, citric acid, or boric acid; and an alkali-resistant micro-.
Claims10
A density controlled cold fusion concrete cementitious spray applied fireproofing formulation comprising:
- from about 5% (wt/wt) to about 30% (wt/wt) of expanded glass 1 mm-2 mm;
- from about 5% (wt/wt) to about 20% (wt/wt) of cenospheres;
- from about 5% (wt/wt) to about 45% (wt/wt) of at least one member including granulated ground blast furnace slag (GGBFS) and Class F Fly Ash;
- from about 3% (wt/wt) to about 15% (wt/wt) of at least one member selected from sodium metasilicate, potassium metasilicate, sodium pentahydrate and potassium pentahydrate;
- from about 0.3% (wt/wt) to about 10.0% (wt/wt) 6 mm glass microfibers;
- from about 0.05% (wt/wt) to about 5.0% (wt/wt) protein;
- and
- from about 5.0% (wt/wt) to about 30% (wt/wt) water.
A density controlled cold fusion concrete cementitious spray applied fireproofing formulation comprising:
- from about 5% (wt/wt) to about 30% (wt/wt) 1 mm-2 mm perlite;
- from about 5% (wt/wt) to about 20% (wt/wt) of cenospheres;
- from about 5% (wt/wt) to about 60% (wt/wt) granulated ground blast furnace slag (GGBFS);
- from about 3% (wt/wt) to about 15% (wt/wt) of at least one member selected from sodium metasilicate, potassium metasilicate, sodium pentahydrate and potassium pentahydrate;
- from about 0.4% (wt/wt) to about 10.0% (wt/wt) 6 mm glass microfibers;
- from about 0.05% (wt/wt) to about 5.0% (wt/wt) protein;
- and
- from about 5.0% (wt/wt) to about 30% (wt/wt) water.