Method of manufacturing thin film polarizer, and thin film polarizer and polarizing plate manufactured using the same
AssigneeLG Chem, Ltd.
InventorsSung Hyun Nam, Jong-Hyun Jung, Kyun-Il Rah, Hye-Min Yu
Life of this patent
Estimating the term…
Abstract
A method of manufacturing a thin film polarizer includes forming a film laminate by allowing a non-oriented polyvinyl alcohol-based film to be bonded to and sandwiched between two or more non-oriented polymer films using attractive force or an adhesive layer, orienting the film laminate so that the polyvinyl alcohol-based film has a thickness of 10 μm or less, and separating the polymer films and the polyvinyl alcohol-based film of the oriented film laminate from each other.
Claims6
A method of manufacturing a thin film polarizer, comprising:
- forming a film laminate by allowing a non-oriented polyvinyl alcohol-based film to be bonded to and sandwiched between two or more non-oriented polymer films using attractive force or an adhesive layer;
- orienting the film laminate so that the polyvinyl alcohol-based film has a thickness of 10 μm or less;
- and
- separating the polymer films and the polyvinyl alcohol-based film of the oriented film laminate from each other,
- wherein adhesion between the polyvinyl alcohol-based film and the polymer film after the orienting of the film laminate is 2N/2 cm or less,
- wherein the non-oriented polymer film comprises one or more selected from a group including a high-density polyethylene film, a polyurethane film, a polypropylene film, a polyolefin film, an ester-based film, a low-density polyethylene film, high-density polyethylene and low-density polyethylene coextrusion films, a copolymer resin film containing ethylene vinyl acetate in high-density polyethylene, an acrylic film, a polyethylene terephthalate film, and a polyvinyl alcohol-based film,
- wherein the orienting of the film laminate is performed through wet orientation at a temperature of 20° C. to 85° C. at an orientation magnification of 5 to 15 times, and
- wherein one or more sheets of thin film polarizer are obtained by separating two or more polymer films and one or more polyvinyl alcohol-based film of the oriented film laminate from each other.
5 more elements