# US 9,637,562 B2 · Processes for recovering rubber from aged briquettes and aged briquettes containing plant matter from non-Hevea plants

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,637,562 B2
- Document ID: US9637562B2
- Status: Granted
- Kind: B2
- Application number: 14/383,380
- Filed: 2013-03-06
- Published: 2015-01-15
- Granted: 2017-05-02
- Earliest claimed: 2012-03-06
- Assignees: Bridgestone Corporation
- Applicants: Bridgestone Corporation
- Inventors: Yingyi Huang; Mark Smale; Robert White; Hiroshi Mouri; William Cole
- Web page: https://patentgrep.com/patent/US9637562B2

## CPC

- C08C 3/02: Purification
- C08C 1/04: Purifying; Deproteinising
- C08C 2/02: Purification
- C08C 2/06: Winning of rubber from solutions
- C08G 83/00: Macromolecular compounds not provided for in groups C08G2/00 - C08G81/00
- C08J 11/08: using selective solvents for polymer components
- C08L 97/02: Lignocellulosic material, e.g. wood, straw or bagasse {(manufacture of articles made from lignocellulosic material by dry processes B27N)}
- C08J 2307/00: Characterised by the use of natural rubber
- C08L 2205/03: containing three or more polymers in a blend
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Provided herein are organic solvent-based processes for the removal of rubber from aged briquettes made from compressed plant matter (briquettes) of non-Hevea plants. Also provided are aged briquettes made from the compressed plant matter of non-Hevea plants where the briquettes have been aged for either various time period after formation and the rubber within the briquette has retained its a molecular weight to within a specified range.

## Claims

### Claim 1

An aged briquette comprising:
78 to 95 weight % compressed chopped plant matter (based upon the total weight of the briquette) from a non-Hevea plant, said plant matter comprising bagasse, rubber, and resin,
2-20 weight % water (based upon the total weight of the briquette),
0.2-2 weight % antioxidant (based upon the total weight of rubber present in the plant matter),
0.1-5 weight % binder (based upon the total weight of the briquette), and
wherein at least 90% of undersize material of less than 30 mesh has been removed from the chopped plant matter prior to briquetting and the briquette has been aged for 18-24 days after formation and the rubber within the briquette has a molecular weight of 1,000,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 2 (depends on 1)

The briquette of claim 1, wherein the rubber within the briquette has a molecular weight of 1,200,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 3 (depends on 1)

The briquette of claim 1, wherein the briquette contains 80-100% by weight bark, less than 20% by weight woody material, and less than 1% by weight leaves.

### Claim 4 (depends on 1)

The briquette of claim 1, wherein the chopped plant matter has an average size of 0.065-0.5″ prior to being compressed into the briquette.

### Claim 5 (depends on 1)

The briquette of claim 1, wherein the chopped plant matter of the briquettes comprises guayule plant matter.

### Claim 6 (depends on 1)

The briquette of claim 1, wherein the briquette has been subjected to further aging for a total aging period of 90-200 days after formation, optionally with at least half of those days at a temperature of 20-50° C., and the rubber within the briquette has a molecular weight of 900,000-1,200,000.

### Claim 7 (depends on 1)

The briquette of claim 1, wherein the amount of the antioxidant is 0.5-2 weight %.

### Claim 8 (depends on 1)

The briquette of claim 1, wherein the chopped plant matter was roll/flake milled prior to being compacted into the briquette.

### Claim 9 (depends on 5)

The briquette of claim 5, wherein the briquette contains 80-100 % by weight bark, less than 20% by weight woody material, and less than 1% by weight leaves.

### Claim 10

An aged briquette comprising:
78 to 95 weight % compressed chopped plant matter (based upon the total weight of the briquette) from a guayule plant, said plant matter comprising bagasse, rubber, and resin,
2-20 weight % water (based upon the total weight of the briquette),
0.2-2 weight % antioxidant (based upon the total weight of rubber present in the plant matter),
0.1-5 weight % binder (based upon the total weight of the briquette),
wherein at least 90% of undersize material of less than 30 mesh has been removed from the chopped plant matter prior to briquetting and the briquette has been aged for 18-24 days after formation and the rubber within the briquette has a molecular weight of 1,000,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 11 (depends on 10)

The briquette of claim 10, wherein the rubber within the briquette has a molecular weight of 1,200,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 12 (depends on 10)

The briquette of claim 10, wherein the briquette contains 80-100% by weight bark, less than 20% by weight woody material, and less than 1% by weight leaves.

### Claim 13 (depends on 10)

The briquette of claim 10, wherein the chopped plant matter has an average size of 0.065-0.5″ prior to being compressed into the briquette.

### Claim 14 (depends on 10)

The briquette of claim 10, wherein the briquette has been subjected to further aging for a total aging period of 90-200 days after formation, optionally with at least half of those days at a temperature of 20-50° C., and the rubber within the briquette has a molecular weight of 900,000-1,200,000.

### Claim 15 (depends on 10)

The briquette of claim 10, wherein the amount of the antioxidant is 0.5-2 weight %.

### Claim 16 (depends on 10)

The briquette of claim 10, wherein the chopped plant matter was roll/flake milled prior to being compacted into the briquette.

### Claim 17 (depends on 11)

The briquette of claim 11, wherein the briquette contains 80-100% by weight bark, less than 20% by weight woody material, and less than 1% by weight leaves.

### Claim 18

An aged briquette comprising:
78 to 95 weight % compressed chopped plant matter (based upon the total weight of the briquette) from a guayule plant, said plant matter comprising bagasse, rubber, and resin,
2-20 weight % water (based upon the total weight of the briquette), and
0.2-2 weight % antioxidant (based upon the total weight of rubber present in the plant matter),
wherein at least 90% of undersize material of less than 30 mesh has been removed from the chopped plant matter prior to briquetting and the briquette has been aged for 18-24 days after formation and the rubber within the briquette has a molecular weight of 800,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 19 (depends on 18)

The briquette of claim 18, wherein the rubber within the briquette has a molecular weight of 1,000,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 20 (depends on 18)

The briquette of claim 18, wherein the rubber within the briquette has a molecular weight of 1,200,000-1,500,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.

### Claim 21 (depends on 18)

The briquette of claim 18, wherein the rubber within the briquette has a molecular weight of 1,000,000-1,200,000, as measured after organic solvent extraction of the rubber from the plant matter of the briquette.