US 9,567,359 B2Granted
Solvent self-reactions with P(CN)3 to produce films and particles of C3N3P
AssigneeThe United States of America as represented by the Secretary of the Navy
InventorsAlbert Epshteyn, Brian L. Chaloux
Life of this patent
Estimating the term…
Abstract
A material with the empirical formula C3N3P is made by polymerizing P(CN)3 in a polar aprotic solvent such as acetonitrile, by heating, irradiation with ultraviolet light, and/or using a polymerization initiator and/or a catalyst.
Claims17
A method of making C3N3P, the method comprising:
- providing, in a sealable vessel, a solution of P(CN)3 in a polar aprotic solvent, and then
- heating the solution to at least 185° C. while the vessel is sealed, thereby obtain a polymer having the empirical formula C3N3P.
A method of making C3N3P, the method comprising:
- providing a starting solution of P(CN)3 in a polar aprotic solvent,
- irradiating the starting solution with ultraviolet light, thereby obtaining a dendrimeric prepolymer comprising C3N3P, and
- separating the prepolymer from the P(CN)3 and solvent.
A method of making C3N3P, the method comprising:
- providing a starting solution of P(CN)3 and a polymerization initiator and/or a catalyst in a polar aprotic solvent;
- heating the solution, thereby obtaining a dendrimeric prepolymer comprising C3N3P;
- and
- separating the prepolymer from the P(CN)3 and solvent.