# US 9,564,333 B2 · Method for forming a metal silicide using a solution containing gold ions and fluorine ions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,564,333 B2
- Document ID: US9564333B2
- Status: Granted
- Kind: B2
- Application number: 14/766,389
- Filed: 2014-02-21
- Published: 2015-12-31
- Granted: 2017-02-07
- Earliest claimed: 2013-02-22
- Assignees: Alchimer
- Applicants: Alchimer
- Inventors: Vincent Mevellec; Dominique Suhr
- Web page: https://patentgrep.com/patent/US9564333B2

## CPC

- H10D 64/0112: {using conductive layers comprising silicides}
- C23C 18/1607: {by direct patterning}
- C23C 18/1639: {Substrates other than metallic, e.g. inorganic or organic or non-conductive}
- C23C 18/1642: {semiconductor (semiconductor H10P14/48)}
- C23C 18/1692: {Heat-treatment}
- C23C 18/1696: {Control of atmosphere}
- C23C 18/1879: {Use of metal, e.g. activation, sensitisation with noble metals}
- C23C 18/1882: {Use of organic or inorganic compounds other than metals, e.g. activation, sensitisation with polymers}
- C23C 18/34: using reducing agents
- C23C 18/36: using hypophosphites
- C23C 18/54: Contact plating, i.e. electroless electrochemical plating
- H10D 64/0131: {the additional conductive layer comprising a silicide layer formed by the silicidation reaction between the layer of silicon with a metal layer which is not formed by metal implantation}
- H10F 77/211: {for photovoltaic cells}
- H10P 14/414: {of metal-silicide materials}
- H10P 14/46: using a liquid
- Y02E 10/50: Photovoltaic [PV] energy
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A subject matter of the invention is a process for the formation of nickel silicide or of cobalt silicide, comprising the stages consisting in: exposing the surface of the silicon-comprising substrate with an aqueous solution comprising from 0.1 mM to 10 mM of gold ions and from 0.6 M to 3.0 M of fluorine ions for a duration of between 5 seconds and 5 minutes, depositing by an electroless route, on the activated substrate, a layer essentially composed of nickel or of cobalt, applying a rapid thermal annealing at a temperature of between 300° C. and 750° C., so as to form the nickel silicide or the cobalt silicide. The aqueous solution comprises a surface-active agent chosen from the compounds comprising at least one anionic or nonionic polar group and an alkyl chain comprising from 10 to 16 carbon atoms. This process essentially has applications in the manufacture of NAND memories and photovoltaic cells.

## Claims

### Claim 1

A process for forming nickel silicide or cobalt silicide on a silicon-comprising substrate, said process comprising the steps of:
bringing a surface of the silicon-comprising substrate into contact with an aqueous solution comprising gold ions and fluoride ions in order to form particles of metallic gold on said surface, wherein the aqueous solution comprises a surface-active agent selected from the group consisting of compounds comprising at least one anionic or one nonionic polar group, and one alkyl chain comprising from 10 to 16 carbon atoms
depositing—by an electroless route—a layer essentially composed of nickel or of cobalt, on the obtained surface covered with particles of metallic gold, wherein the thickness of the layer is between 10 and 45 nm, and the variation in the thickness of the layer is less than 10%, and
applying a rapid thermal annealing at a temperature of between 300° C. and 750° C., so as to form nickel silicide or cobalt silicide.

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein the surface of the silicon-comprising substrate is brought into contact with the aqueous solution for a duration of between 5 seconds and 5 minutes.

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein the aqueous solution comprising fluoride ions is obtained by a step of incorporating hydrofluoric acid (HF), NH4F, or one of their mixtures, into water.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the aqueous solution comprising gold ions is obtained by a step of incorporating chloroauric acid (HAuCl4) into water.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the aqueous solution comprises:
from 0.1 mM to 10 mM of gold ions, and
from 0.6 M to 3.0 M of fluoride ions.

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein the alkyl chain comprises from 10 to 14 carbon atoms.

### Claim 7 (depends on 1)

The process as claimed in claim 1, wherein the layer essentially composed of nickel or of cobalt is a nickel-boron layer that is obtained by a step of bringing into contact said surface covered with particles of metallic gold with an aqueous solution comprising a nickel salt, a boron-based reducing agent, a stabilizing agent for nickel, and a polyamine, the pH of the solution being between 9 and 12 and the temperature of the aqueous solution being between 50° C. and 90° C.

### Claim 8 (depends on 1)

The process as claimed in claim 1, further comprising a step of chemical cleaning of nickel silicide or cobalt silicide, so as to remove nickel or cobalt which has not migrated into the silicon at the end of the rapid thermal annealing stage.

### Claim 9 (depends on 1)

The process as claimed in claim 1, wherein the rapid thermal annealing temperature ranges from 350° C. to 450° C.

### Claim 10 (depends on 1)

The process as claimed in claim 1, wherein the surface-active agent has a molecular weight of between 100 g/mol and 1500 g/mol.

### Claim 11 (depends on 1)

The process as claimed in claim 1, wherein the surface-active agent comprises an anionic polar group.

### Claim 12 (depends on 10)

The process as claimed in claim 10, wherein the surface-active agent is sodium dodecylsulfate.

### Claim 13 (depends on 1)

A process for the manufacture of a NAND memory comprising a process for the formation of nickel silicide or of cobalt silicide as defined in claim 1.

### Claim 14 (depends on 1)

A process for the manufacture of photovoltaic cells comprising a process for the formation of nickel silicide or of cobalt silicide as defined in claim 1.

### Claim 15 (depends on 1)

A process according to claim 1, wherein the thickness of the layer is between 10 and 25 nm.

### Claim 16 (depends on 1)

A process according to claim 1, wherein the variation in the thickness of the layer is less than 5%.

### Claim 17

A process for forming a layer that is essentially composed of nickel or of cobalt on a silicon-comprising substrate, said process comprising the steps of:
exposing a surface of the silicon-comprising substrate with an aqueous solution comprising gold ions, fluoride ions and a surface-active agent chosen in the group consisting of compounds comprising at least one anionic or nonionic polar group, and one alkyl chain comprising from 10 to 16 carbon atoms, so as to activate the said surface of the silicon-comprising substrate, and
depositing—by an electroless route—on the activated surface of the silicon-comprising substrate, a layer essentially composed of nickel or of cobalt that has a thickness between 10 and 45 nm, the variation in the thickness of the layer being less than 10%.

### Claim 18 (depends on 17)

A process according to claim 17, wherein the thickness of the layer is between 10 and 25 nm.

### Claim 19 (depends on 17)

A process according to claim 17, wherein the variation in the thickness of the layer is less than 5%.