Iron-based alloys and methods of making and use thereof
AssigneeL.E. Jones Company
InventorsCong Yue Qiao, Peter Vennema, Douglas W. Dooley, David Doll
Life of this patent
Estimating the term…
Loading patent…
AssigneeL.E. Jones Company
InventorsCong Yue Qiao, Peter Vennema, Douglas W. Dooley, David Doll
Estimating the term…
An iron-based alloy includes, in weight percent, carbon from about 2 to about 3 percent; manganese from about 0.1 to about 0.4 percent; silicon from about 0.3 to about 0.8 percent; chromium from about 11.5 to about 14.5 percent; nickel from about 0.05 to about 0.6 percent; vanadium from about 0.8 to about 2.2 percent; molybdenum from about 4 to about 7 percent; tungsten from about 3 to about 5 percent; niobium from about 1 to about 3 percent; cobalt from about 3 to about 5 percent; boron from zero to about 0.2 percent; and the balance containing iron and incidental impurities. The alloy is suitable for use in elevated temperature applications such as in valve seat inserts for combustion engines.
An iron-based alloy comprising, in weight percent:
A valve seat insert for use in an internal combustion engine, the valve seat insert made of an iron-based alloy comprising, in weight percent:
Dependencies are inferred from the claim text.