Method of ore processing
AssigneeThe University of Queensland
InventorsJames Vaughan, William Hawker
Life of this patent
Estimating the term…
Abstract
A method of selectively leaching a metal such as nickel from an ore or ore processing intermediate comprising the metal and cobalt. The ore or ore processing intermediate is contacted with an acidic leach solution comprising an amount of an oxidising agent sufficient to oxidise a major portion of the cobalt to thereby cause it to be stabilised in the solid phase while a major portion of the metal is dissolved for subsequent recovery.
Claims20
A method of selectively leaching a metal selected from the group consisting of nickel, copper and zinc from a solid ore or solid ore processing intermediate comprising the metal and cobalt, the method including:
- providing a mixture comprising an acidic leach solution and an oxidizing agent;
- and
- mixing the mixture with the solid ore or solid ore intermediate,
- wherein there is sufficient oxidizing agent to stabilize a substantial portion of the cobalt to cause it to be stabilized in a solid phase while greater than 95% by mass of the metal is selectively dissolved.
A method of recovering nickel and cobalt from a mixed nickel-cobalt hydroxide precipitate including:
- (a) providing a mixture comprising an acidic leach solution and an oxidizing agent, wherein there is sufficient oxidizing agent to stabilize a substantial portion of the cobalt to cause it to be stabilized in a solid phase while greater than 95% by mass of the nickel is selectively dissolved;
- (b) mixing the mixture with the mixed nickel-cobalt hydroxide precipitate;
- (c) separating the cobalt in the solid phase from the acidic leach solution containing dissolved nickel to recover the cobalt in the solid phase;
- and
- (d) recovering the nickel from the acidic leach solution.
A method of selectively leaching a metal selected from the group consisting of nickel, copper and zinc from a solid ore or solid ore processing intermediate comprising the metal and cobalt, the method including:
- a) providing a mixture comprising an acidic leach solution and an oxidizing agent;
- and
- b) mixing the mixture with the solid ore or solid ore processing intermediate,
- wherein there is sufficient oxidizing agent to stabilize a substantial portion of the cobalt to cause it to be stabilized in a solid phase while greater than 95% by mass of the metal is selectively dissolved within 5 hours.
Dependencies are inferred from the claim text.