# US 9,378,957 B2 · Silicon substrates with doped surface contacts formed from doped silicon based inks and corresponding processes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,378,957 B2
- Document ID: US9378957B2
- Status: Granted
- Kind: B2
- Application number: 14/180,600
- Filed: 2014-02-14
- Published: 2014-06-12
- Granted: 2016-06-28
- Earliest claimed: 2011-01-31
- Assignees: NanoGram Corporation
- Applicants: NanoGram Corporation
- Inventors: Guojun Liu; Uma Srinivasan; Shivkumar Chiruvolu
- Web page: https://patentgrep.com/patent/US9378957B2

## CPC

- H10P 32/171: {being group IV material}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10P 32/1404: {using predeposition followed by drive-in of impurities into the semiconductor surface, e.g. predeposition from a gaseous phase}
- H10P 32/16: between a solid phase and a liquid phase
- H10P 32/19: {Diffusion sources}
- Y02E 10/52: PV systems with concentrators
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The use of doped silicon nanoparticle inks and other liquid dopant sources can provide suitable dopant sources for driving dopant elements into a crystalline silicon substrate using a thermal process if a suitable cap is provided. Suitable caps include, for example, a capping slab, a cover that may or may not rest on the surface of the substrate and a cover layer. Desirable dopant profiled can be achieved. The doped nanoparticles can be delivered using a silicon ink. The residual silicon ink can be removed after the dopant drive-in or at least partially densified into a silicon material that is incorporated into the product device. The silicon doping is suitable for the introduction of dopants into crystalline silicon for the formation of solar cells.

## Claims

### Claim 1

A dopant source composition comprising of a solvent, from about 2.5 weight percent to about 40 weight percent of a glass/ceramic precursor composition wherein the glass/ceramic precursor composition comprises a precursor for glass/ceramic oxide, nitride, carbide or combinations thereof, and from about 0.1 wt % to about 20 wt % doped particles selected from the group consisting of doped silicon nanoparticles, doped silica nanoparticles or a combination thereof.

### Claim 2 (depends on 1)

The dopant source composition of claim 1 wherein the glass/ceramic precursor composition comprises a spin-on glass composition.

### Claim 3 (depends on 1)

The dopant source composition of claim 1 wherein the glass/ceramic precursor composition comprises a sol-gel that thermally converts to a metal/metalloid oxide.

### Claim 4 (depends on 1)

The dopant source composition of claim 1 comprising silicon nanoparticles.

### Claim 5 (depends on 1)

The dopant source composition of claim 1 wherein the silicon nanoparticles have average primary particle diameter from about 1 nm to about 75 nm.

### Claim 6 (depends on 1)

The dopant source composition of claim 1 wherein the solvent comprises an alcohol.

### Claim 7 (depends on 1)

The dopant source composition of claim 1 wherein the doped particles comprise doped silicon particles.

### Claim 8 (depends on 1)

The dopant source composition of claim 1 further comprising N-methyl pyrrolidone, terpineol, 2-(2-ethoxyethoxy)ethanol (Carbitol), butyl cellosolve, or combinations thereof.

### Claim 9 (depends on 1)

The dopant source composition of claim 1 comprising a blend of doped silicon nanoparticles and doped silica nanoparticles.

### Claim 10

A method for doping a silicon substrate, the method comprising:
depositing using screen printing a dopant source composition to form a doped deposit on the silicon substrate, wherein the dopant source composition comprises a blend of a solvent, an undoped glass/ceramic precursor composition, and doped particles selected from the group consisting of doped silicon nanoparticles, doped silica nanoparticles or a combination thereof; and
heating the silicon substrate to drive the dopant element into the silicon substrate.

### Claim 11 (depends on 10)

The method of claim 10 further comprising the performance of an initial heating step to cure the glass/ceramic precursor composition prior to performing the dopant drive in heating step.

### Claim 12 (depends on 11)

The method of claim 11 wherein the initial heating step is performed at a temperature from about 300° C. to about 800° C.

### Claim 13 (depends on 10)

The method of claim 10 further comprising etching the silicon substrate after performing the dopant drive-in to substantially remove remaining depleted dopant source composition.

### Claim 14 (depends on 10)

The method of claim 10 wherein the heating to drive-in dopant atoms into the silicon substrate is performed at a temperature from about 650° C. to about 1300° C.

### Claim 15 (depends on 10)

The method of claim 10 wherein the doped substrate after heating has dopant driven into the silicon substrate to depth from about 0.5 microns to 2.5 microns at a dopant concentration of 1×1019 atoms/cm3.

### Claim 16 (depends on 10)

The method of claim 10 wherein the heating to perform dopant drive in is performed in a substantially oxygen free atmosphere.

### Claim 17 (depends on 10)

The method of claim 10 wherein the heating step is performed in an oven.

### Claim 18 (depends on 10)

The method of claim 10 wherein the silicon sheet after performing to drive in dopant has a sheet resistance of no more than about 120 ohms/square.