# US 9,368,397 B2 · Method for forming a vertical electrical connection in a layered semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,368,397 B2
- Document ID: US9368397B2
- Status: Granted
- Kind: B2
- Application number: 14/119,184
- Filed: 2012-05-22
- Published: 2014-03-27
- Granted: 2016-06-14
- Earliest claimed: 2011-05-23
- Assignees: Alchimer
- Applicants: Dominique Suhr; Vincent Mevellec
- Inventors: Dominique Suhr; Vincent Mevellec
- Web page: https://patentgrep.com/patent/US9368397B2

## CPC

- H10W 20/089: {using processes for implementing desired shapes or dispositions of the openings, e.g. double patterning}
- H10P 14/46: using a liquid
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- H10P 50/283: {by chemical means}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10W 20/023: {the interconnections being through-semiconductor vias}
- H10W 20/0234: {comprising etching via holes that stop on pads or on electrodes}
- H10W 20/0242: {comprising etching via holes from the back sides of the chips, wafers or substrates}
- H10W 20/0265: {characterised by the sidewall insulation}
- H10W 20/044: {for electroless plating}
- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/076: {in via holes or trenches}
- H10W 20/094: {by transforming insulators into conductors}
- H10W 20/20: Interconnections within wafers or substrates, e.g. through-silicon vias [TSV]
- H10W 20/2125: {Top-view shapes}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/435: {Cross-sectional shapes or dispositions of interconnections}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The invention proposes a method for forming a vertical electrical connection (50) in a layered semiconductor structure (1), comprising the following steps: —providing (100) a layered semiconductor structure (1), said layered semiconductor structure (1) comprising: —a support substrate (20) including an first surface (22) and a second surface (24), —an insulating layer (30) overlying the first surface (22) of the support substrate (20), and —at least one device structure (40) formed in the insulating layer (30); and —drilling (300) a via (50) from the second surface of the support substrate (20) up to the device structure (40), in order to expose the device structure (40); characterized in that drilling (300) of the insulating layer is at least performed by wet etching (320).

## Claims

### Claim 1

A method for forming a vertical electrical connection in a layered semiconductor structure, comprising the following steps:
providing a layered semiconductor structure, said layered semiconductor structure comprising:
a support substrate including a first surface and a second surface,
an insulating layer overlying the first surface of the support substrate, and
at least one device structure formed in the insulating layer; and
drilling a via from the second surface of the support substrate up to the device structure, in order to expose the device structure, drilling of the insulating layer being at least partially performed by wet etching;
wet coating the via with an insulating film by bringing a surface of said via into contact with a liquid solution, in order to obtain a uniform insulating film, wherein the wet coating of the via is selective and only coats the via in the vicinity of the support substrate and preparing a copper diffusion barrier by forming by a wet process, at the surface of the insulating film, an organic film containing particles of metals or metal alloys.

### Claim 2 (depends on 1)

The method of claim 1, wherein wet etching is performed during a predetermined time, said predetermined time depending on the material of the insulating layer, the etchant and the thickness of the insulating layer to be drilled.

### Claim 3 (depends on 1, 2)

The method of claim 1 or 2, wherein wet etching is performed with a solution containing fluorhydric acid, and optionally glycerol.

### Claim 4 (depends on 3)

The method of claim 3, wherein the etchant comprises between 0.5% and 50% in volume of Fluorhydric acid, preferably 1.35%.

### Claim 5 (depends on 3, 4)

The method of claim 3 or 4, wherein the etchant further comprises between 0.5 and 50% in volume of glycerol, preferably 1.35%.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The method of anyone of claims 1 to 5 further comprising a pre-wetting step prior to the wet etching step, wherein the layered semiconductor structure is plunged in water.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

The method of anyone of claims 1 to 6 further comprising a rinsing step following the wet etching step, wherein the layered semiconductor structure is rinsed with water.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The method of anyone of claims 1 to 7 further comprising a vacuum step following the wet etching step, wherein the layered semiconductor structure is submitted to a controlled vacuum.

### Claim 9 (depends on 8)

The method of claim 8, wherein the layered semiconductor structure is plunged in water during the vacuum step.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

The method of anyone of claims 1 to 9 further comprising a removal step before the wet etching step, wherein the support substrate is thinned.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The method of anyone of claims 1 to 10 further comprising a pre-drilling step before the wet etching step, wherein a pre via is formed from the second surface up to at least the insulating layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the pre via is formed by dry etching, wet etching or reactive ion etching.

### Claim 13 (depends on 1)

The method of claim 1, wherein the solution comprises:
a protic solvent;
at least one diazonium salt;
at least one monomer that is chain-polymerizable and soluble in said protic solvent;
at least one acid in a sufficient quantity to stabilize said diazonium salt by adjusting the pH of said solution to a value less than 7, preferably less than 2.5; and
wherein the surface of said vertical connection is polarizes according to a potentio- or galvano-pulsed mode for a duration sufficient to form a film having a thickness of at least 60 nanometers, and preferably between 80 and 500 nanometers.

### Claim 14 (depends on 1)

The method of claim 1, wherein the particles of metal or metal alloys of the organic film may comprise nanoparticles wherein the metal or metal alloy may comprise and the step of preparation of the copper diffusion barrier further comprises, nickel or cobalt;
bringing the film thus formed into contact with a liquid solution containing at least one metal salt, preferably of the same nature as the metal incorporated into the organic film, a stabilizing agent, and at least one reducing agent under conditions enabling the formation of a metal film having a thickness of at least 100 nm.

### Claim 15 (depends on 1)

The method of claim 1, further comprising the preparation of a copper diffusion barrier by:
1. activating the surface of the insulating layer with a solution comprising:
i) an activator constituted of one or several palladium complexes chosen in the group consisting of:
palladium complexes having the formula:
wherein:
R1 and R2 are identical and represent H; CH2CH2NH2; CH2CH2OH; or
R1 represents H and R2 represents CH2CH2NH2; or
R2 represents CH2CH2NHCH2CH2NH2 and R1 represents CH2CH2NH2; or
R2 represents CH2CH2NHCH2CH2NHCH2CH2NH2 and R1 represents H;
X represents a ligand chosen in the group consisting of Cl−; Br−; I−; H2O, NO3−; CH3SO3−; CF3SO3−; CH3-Ph-SO3−; CH3COO−;
palladium complexes having the formula or:
wherein:
R1 and R2 are defined as above-mentioned, and
Y represents a counter-ion comprising two negative charges constituted:
either of two mono-anions preferably chosen in the group consisting of Cl−; PF6−; BF4−; NO3−; CH3SO3−; CF3SO3−; CH3C6H4SO3; CH3COO−; or
of a di-anion, preferably SO42−;
ii) an bi-functional organic binder constituted of one or several organosilanes having the general formula:
{NH2-(L)}3-n-Si(OR)n
wherein:
L is a spacer selected from the group consisting of CH2; CH2CH2; CH2CH2CH2— and CH2CH2NHCH2CH2;
R is a group selected from the group consisting of CH3, CH3CH2, CH3CH2CH2, 2CH; and
n is an integer equal to 1, 2 or 3,
iii) a solvent system constituted of one or several solvents suitable for solubilising said activator and said binder;
2. electrolessly depositing a metallic layer on the activated surface.

### Claim 16 (depends on 14, 15)

The method of claim 14 or 15, further comprising the preparation of a copper seed layer by:
a) bringing the free surface of the copper diffusion barrier layer into contact with a liquid solution comprising:
at least one solvent;
copper ions in a concentration of between approximately 14 and 120 mM;
ethylenediamine;
the molar ratio of ethylenediamine to copper being between 1.80 and 2.03;
the pH of said composition being between 6.6 and 7.5;
b) polarizing said free surface of the second layer for a sufficient duration to form said copper seed layer.

### Claim 17 (depends on 16)

The method of claim 16, further comprising a step of metallization of the vertical electrical connection by electrodepositing copper with a composition comprising:
copper ions, said copper ions having a concentration of 45 to 1500 mM, preferably 45 to 500 mM, and more preferably 100 to 300 mM;
a complexing agent for copper, comprising at least one component of the group comprising the aliphatic polyamines having 2 to 4 amino groups, said complexing agent for copper having a concentration of 45 to 3000 mM, preferably 45 to 1500 mM, and more preferably 300 to 900 mM;
the molar ratio between copper and said complexing agent for copper being of 0.1 to 5, preferably 0.1 to 1, and more preferably 0.2 to 0.4;
thiodiglycolic acid, said thiodiglycolic acid having a concentration of 1 to 500 mg/L; and
optionally, a buffering system, in particular ammonium sulphate, in a concentration of 0.1 to 3 M.

### Claim 18

A method for forming a vertical electrical connection in a layered semiconductor structure, comprising the following steps:
providing a layered semiconductor structure, said layered semiconductor structure comprising:
a support substrate including a first surface and a second surface,
an insulating layer overlying the first surface of the support substrate, and
at least one device structure formed in the insulating layer; and
drilling a via from the second surface of the support substrate up to the device structure, in order to expose the device structure, drilling of the insulating layer being at least partially performed by wet etching;
wet coating the via with an insulating film by bringing a surface of said via into contact with a liquid solution, in order to obtain a uniform insulating film, wherein the wet coating of the via is selective and only coats the via in the vicinity of the support substrate,
wherein the solution comprises:
a protic solvent;
at least one diazonium salt;
at least one monomer that is chain-polymerizable and soluble in said protic solvent; and
at least one acid in a sufficient quantity to stabilize said diazonium salt by adjusting the pH of said solution to a value less than 7, preferably less than 2.5.

### Claim 19 (depends on 18)

The method of claim 18, wherein the surface of said vertical connection is polarized according to a potentio- or galvano-pulsed mode for a duration sufficient to form a film having a thickness of at least 60 nanometers, and preferably between 80 and 500 nanometers.

### Claim 20

A method for forming a vertical electrical connection in a layered semiconductor structure, comprising the following steps:
providing a layered semiconductor structure, said layered semiconductor structure comprising:
a support substrate including a first surface and a second surface
an insulating layer overlying the first surface of the support substrate, and
at least one device structure formed in the insulating layer; and
drilling a via from the second surface of the support substrate up to the device structure, in order to expose the device structure, drilling of the insulating layer being at least partially performed by wet etching;
wet coating the via with an insulating film by bringing a surface of said via into contact with a liquid solution, in order to obtain a uniform insulating film, wherein the wet coating of the via is selective and only coats the via in the vicinity of the support substrate, and
preparing a copper diffusion barrier by activating the surface of the insulating layer with a solution comprising:
i) an activator constituted of one or several palladium complexes,
ii) an bi-functional organic binder,
iii) a solvent system constituted of one or several solvents suitable for solubilizing said activator and said binder.

### Claim 21 (depends on 20)

The method of claim 20, wherein:
i) the one or several palladium complexes are chosen in the group consisting of:
palladium complexes having the formula:
R1 N N R2
Pd
X X (I)
wherein:
R1 and R2 are identical and represent H; CH2CH2NH2; CH2CH2OH; or
R1 represents H and R2 represents CH2CH2NH2; or
R2 represents CH2CH2NHCH2CH2NH2 and R1 represents CH2CH2NH2; or
R2 represents CH2CH2NHCH2CH2NHCH2CH2NH2 and R1 represents H;
X represents a ligand chosen in the group consisting of Cl—; Br—; I—; H2O, NO3-; CH3SO3-; CF3SO3-; CH3-Ph-SO3-; CH3COO—;
palladium complexes having the formula or:
Y2-
Y2-
R1 N N R2
R1 N N R2
Pd
R2 N N R1
R1 N N R2
Pd
(IIa) (IIb)
2+
wherein:
R1 and R2 are defined as above-mentioned, and
Y represents a counter-ion comprising two negative charges constituted:
either of two mono-anions preferably chosen in the group consisting of Cl—; PF6-; BF4-; NO3-; CH3SO3-; CF3SO3-; CH3C6H4SO3-; CH3COO—; or
of a di-anion, preferably SO42−;
ii) the bi-functional organic binder is constituted of one or several organosilanes having the general formula:
{NH2-(L)}3-n-Si(OR)n
wherein:
L is a spacer selected from the group consisting of CH2; CH2CH2; CH2CH2CH2- and CH2CH2NHCH2CH2;
R is a group selected from the group consisting of CH3, CH3CH2, CH3CH2CH2, 2CH; and
n is an integer equal to 1, 2 or 3, and the step of preparation of the copper diffusion barrier further comprises electrolessly depositing a metallic layer on the activated surface.