# US 9,357,657 B2 · Lead-free solder alloy for printed circuit board assemblies for high-temperature environments

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,357,657 B2
- Document ID: US9357657B2
- Status: Granted
- Kind: B2
- Application number: 14/814,015
- Filed: 2015-07-30
- Published: 2015-11-19
- Granted: 2016-05-31
- Earliest claimed: 2015-07-30
- Assignees: Halliburton Energy Services, Inc.
- Applicants: Halliburton Energy Services, Inc.
- Inventors: Andrew Albert Hrametz; Alexander T. Duncan
- Web page: https://patentgrep.com/patent/US9357657B2

## CPC

- H05K 3/346: Solder materials or compositions specially adapted therefor
- B23K 35/262: {Sn as the principal constituent}
- C22C 13/00: Alloys based on tin
- C22C 13/02: with antimony or bismuth as the next major constituent
- E21B 49/00: Testing the nature of borehole walls; Formation testing; Methods or apparatus for obtaining samples of soil or well fluids, specially adapted to earth drilling or wells
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A solder alloy suitable for high temperature environments, such as for example electronic systems used in an oil or gas well where the temperature may be in the region of 175° C., the solder alloy having a Silver weight % in the range of 3.5 to 7.0, a Copper weight % in the range of 1.0 to 4.0, and an Antimony weight % in the range of 1.0 to 3.0. Other embodiments are described and claimed.

## Claims

### Claim 1

A well logging tool comprising:
an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition consisting of:
Silver;
Copper;
Antimony; and
Tin;
wherein the preliminary solid solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, and a weight % of the Antimony in a range of 1.0 to 3.0.

### Claim 2 (depends on 1)

The well logging tool as set forth in claim 1, wherein the preliminary solid solder alloy has 4.7 weight % Silver, 1.7 weight % Copper, and 1.5 weight % Antimony.

### Claim 3

A well logging tool comprising:
an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition consisting of:
Silver;
Copper;
Antimony;
Zinc; and
Tin;
wherein the preliminary solid solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, a weight % of the Antimony in a range of 1.0 to 3.0; and a weight % of the Zinc in a range of 0.1 to 1.0.

### Claim 4 (depends on 3)

The well logging tool as set forth in claim 3, wherein the preliminary solid solder alloy has 4.7 weight % Silver, 1.7 weight % Copper, and 1.5 weight % Antimony.

### Claim 5

A well logging tool comprising:
an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition comprising:
Silver;
Copper;
Antimony; and
Tin;
wherein the solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, a weight % of the Antimony in a range of 1.0 to 3.0, and the remainder Tin.

### Claim 6 (depends on 5)

The well logging tool as set forth in claim 5, wherein the preliminary solid solder alloy composition comprises about 4.7 weight % Silver, about 1.7 weight % Copper, about 1.5 weight % Antimony, and the remainder Tin.

### Claim 7 (depends on 6)

The well logging tool as set forth in claim 6, wherein the preliminary solid solder composition further comprises Zinc.

### Claim 8 (depends on 7)

The well logging alloy as set forth in claim 7, wherein the preliminary solid solder alloy composition has a weight % of the Zinc in a range of 0.1 to 1.0.

### Claim 9 (depends on 8)

The well logging tool as set forth in claim 8, wherein the preliminary solid solder alloy composition has a weight % of the Tin in a range of 85.0 to 94.4.

### Claim 10 (depends on 5)

The well logging tool as set forth in claim 5, wherein the preliminary solid solder alloy composition has a weight % of the Tin in a range of 86.0 to 94.5.

### Claim 11 (depends on 5)

The well logging tool as set forth in claim 5, wherein the preliminary solid solder alloy composition further comprises at least 0.1 weight % Zinc.

### Claim 12 (depends on 11)

The well logging tool as set forth in claim 11, wherein the preliminary solid solder alloy composition comprises a weight % of the Zinc in a range of 0.1 to 1.0.