# US 9,356,313 B2 · Solid electrolyte for lithium battery, comprising at least one zone of lithium-containing glass ceramic material and method of production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,313 B2
- Document ID: US9356313B2
- Status: Granted
- Kind: B2
- Application number: 14/117,238
- Filed: 2012-06-15
- Published: 2014-09-04
- Granted: 2016-05-31
- Earliest claimed: 2011-06-16
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Sami Oukassi; Samir Guerroudj; Michaël Roffat
- Inventors: Sami Oukassi; Samir Guerroudj; Michaël Roffat
- Web page: https://patentgrep.com/patent/US9356313B2

## CPC

- H01M 10/052: Li-accumulators
- H01M 6/185: {with oxides, hydroxides or oxysalts as solid electrolytes}
- H01M 6/187: {Solid electrolyte characterised by the form}
- H01M 6/40: Printed batteries {, e.g. thin film batteries}
- H01M 10/0562: Solid materials
- H01M 2300/0071: Oxides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

At least one zone made of lithium-containing glass-ceramic material, in a solid electrolyte for a lithium battery, is formed from a lithium-containing ceramic material, advantageously in the form of a layer such as a thin film. It is obtained by melting of at least a part of the lithium-containing ceramic material, followed by a recrystallization heat treatment. Melting is obtained by a laser beam irradiation operation, which enables fabrication of the solid electrolyte to be performed directly on a multilayer stack comprising certain active components of the lithium battery.

## Claims

### Claim 1

A method for producing a solid electrolyte for a lithium battery comprising at least one zone made from lithiated glass-ceramic material, wherein the lithiated glass-ceramic material zone is achieved by melting of at least a part of a lithiated ceramic material, performed by a laser beam irradiation operation and followed by a recrystallization heat treatment.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, before the laser beam irradiation operation, the lithiated ceramic material is in the form of a layer.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the layer presents a compactness comprised between 70% and 95% and advantageously between 85% and 95%.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the layer is a thin film.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the thin film is formed on a support, before the laser beam irradiation operation.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the support is a multilayer stack comprising at least one current collector and an electrode for a lithium battery.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the whole of the thin film is subjected to the laser beam irradiation operation.

### Claim 8 (depends on 2)

The method according to claim 2, wherein the layer is a bulk substrate.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the bulk substrate is locally subjected to the laser beam irradiation operation, the part of the bulk substrate subjected to the laser beam irradiation operation forming the lithiated glass-ceramic material zone of the solid electrolyte, after the recrystallization heat treatment.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the laser beam is a pulsed laser beam.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the recrystallization heat treatment is performed in a furnace at a lower temperature than the melting temperature of the lithiated ceramic material, for a time comprised between 1 hour and 72 hours.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the recrystallization heat treatment is performed by an additional laser beam irradiation operation.

### Claim 13 (depends on 1)

A solid electrolyte for a lithium battery produced by the method of claim 1, comprising at least one lithiated glass-ceramic material zone, and at least one additional zone constituted by grains of lithiated ceramic material coated by the lithiated glass-ceramic material, said additional zone being in contact with the lithiated glass-ceramic material zone.