# US 9,356,288 B2 · Transition metal composite hydroxide and lithium composite metal oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 9,356,288 B2
- Document ID: US9356288B2
- Status: Granted
- Kind: B2
- Application number: 13/700,916
- Filed: 2011-06-09
- Published: 2013-05-23
- Granted: 2016-05-31
- Earliest claimed: 2010-06-17
- Assignees: Sumitomo Chemical Company, Limited
- Applicants: Kenji Takamori; Hiroshi Inukai; Taiga Obayashi
- Inventors: Kenji Takamori; Hiroshi Inukai; Taiga Obayashi
- Web page: https://patentgrep.com/patent/US9356288B2

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/84: Hydroxides
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- C01P 2002/54: one element only
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/40: Electric properties
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/52: of nickel, cobalt or iron
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 6/185: {with oxides, hydroxides or oxysalts as solid electrolytes}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/109: of button or coin shape
- H01M 50/186: characterised by the disposition of the sealing members
- H01M 50/443: Particulate material
- H01M 2004/028: {Positive electrodes}
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- H01M 2300/004: Three solvents
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

Provided are a transition metal mixed hydroxide comprising an alkali metal other than Li, SO4 and a transition metal element, wherein the molar ratio of the molar content of the alkali metal to the molar content of the SO4 is not less than 0.05 and less than 2, and a lithium mixed metal oxide obtained by calcining a mixture of the transition metal mixed hydroxide and a lithium compound by maintaining the mixture at a temperature of 650 to 1000° C.

## Claims

### Claim 1

A transition metal mixed hydroxide containing an alkali metal other than Li, SO4 and a transition metal element, wherein the molar ratio of the molar content of all of the alkali metal other than Li to the molar content of the SO4 is not less than 1 and less than 2, and the molar ratio of the molar content of the alkali metal to the molar content of the transition metal mixed hydroxide is 0.00001 to 0.003.

### Claim 2 (depends on 1)

The transition metal mixed hydroxide according to claim 1, wherein the transition metal element represents Ni, Mn and Fe.

### Claim 3 (depends on 2)

The transition metal mixed hydroxide according to claim 2, wherein the molar ratio of Ni:Mn:Fe is (1−x−y):x:y, wherein x is not less than 0.3 and not more than 0.7 and y is more than 0 and less than 0.2.

### Claim 4 (depends on 1)

The transition metal mixed hydroxide according to claim 1, wherein the alkali metal is K.

### Claim 5 (depends on 1)

A method for producing a lithium mixed metal oxide, the method comprising calcining a mixture of the transition metal mixed hydroxide according to claim 1 and a lithium compound by maintaining the mixture at a temperature of 650 to 1000° C.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the transition metal mixed hydroxide is obtained by a method comprising the following steps (1) and (2):
(1) a step of bringing an aqueous solution containing a transition metal element and SO4 into contact with an alkali comprising an alkali metal other than Li to obtain a coprecipitate slurry,
(2) a step of obtaining a transition metal mixed hydroxide from the coprecipitate slurry.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the aqueous solution is an aqueous solution obtained by dissolving a sulfate of Ni, a sulfate of Mn and a sulfate of Fe in water.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the sulfate of Fe is a sulfate of divalent Fe.